Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants 748S-UV (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8182 (837) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8182R (837RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8190 (483) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8623 (717C) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8623G (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Temperature at which stiffness does not exceed 70 Mpa |
Precision Polymer Engineering N50M Nitrile Rubber Nitrile Butadiene Rubber, 48-58 °IRHD. Medium acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Standard BS2751 BA50.Applications: Excellent resistance to petro.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Temperature at which stiffness does not exceed 70 Mpa |
Precision Polymer Engineering N70N Nitrile Rubber Nitrile Butadiene Rubber (NBR) 66-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD5595A Grade 70.Applications: Synthetic rubber resistant to petrole.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | ASTM D2137, Non-brittle after 3 minutes |
Precision Polymer Engineering V72H Fluoroelastomer Compound Fluoroelastomer Rubber, 65-75 °IRHD. FDA grade. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Admi.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Precision Polymer Engineering Z95X Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR.Applications: Gas blister resistant compound designed for use in applica.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Flex TR10; ASTM D1329 |
Parker Chomerics CHO-SEAL V6433 Conductive Elastomer Material of choice for extensive fluid resistance; no corrosion resistance.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Butyl Rubber (IIR, CIIR, BIIR) Butyl rubber is a copolymer of isoprene (minor) and isobutylene. Chlorobutyl (CIIR) and Bromobutyl (BIIR) contains 1.2% of the halogen. The halogen addition changes the cure characteristics and ca.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit V60 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit V60WH Non-Black Compound Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit V75BR Non-Black Compound Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit Simriz® 482 Low Temperature FFKT Perfluoroelastomer Compound Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of .. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit V75 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Gehman T100 |
Zeon Chemicals HyTemp® AR22 AR Super ACM Polyacrylate Elastomer Monomer composition is optimized for improved tensile strength and oil resistance over traditional acrylates. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg Commercial Neoprene® C798 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg R608 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg R661 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Chesterton 610 HT Synthetic Lubricating Fluid Description: Chesterton® 610 HT Synthetic Lubrication Fluid is a premium quality full synthetic lubricant designed to provide lubrication at temperatures ranging from -25°C (-15°F) for those over.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Chesterton 610 MT Plus Synthetic Lubricating Fluid Description: Chesterton® 610 MT Plus Synthetic Lubricating Fluid is a premium quality full synthetic lubricant designed to provide lubrication at temperatures ranging from 25°C (-15°F) to those o.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Gehman torsion test, T2 |
Daikin DAI-EL LT-302 Fluoroelastomer, Low Temperature Grade, 64% Fluorine Content Features: Flexible up to -30°C, excellent low temperature sealing.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | JIS-K-6723 |
Denka VINYKON M2510 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | JIS-K-6723 |
Denka VINYKON W5120 PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
ATG s.r.l. AU-EU Polyurethane Rubber |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg R660 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg Z600 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |