Category | Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE) |
Manufacturer | ATG s.r.l. |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | ATG s.r.l. AU-EU Polyurethane Rubber.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.15 g/cc | 1.15 g/cc |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 50 - 95 | 50 - 95 | |
Tensile Strength, Ultimate | 15.0 - 35.0 MPa | 2180 - 5080 psi | |
Elongation at Break | 250 - 700 % | 250 - 700 % | |
Rebound | 35 - 50 % | 35 - 50 % |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 110 °C | 230 °F | |
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Abrasion Resistance | high | |
Chemical Resistance to Animal and Vegetable Oils and Greases | high | |
Chemical Resistance to Aromatic Hydrocarbons | medium | |
Chemical Resistance to Chloride Solvents | low | |
Chemical Resistance to Distilled Water | low | |
Chemical Resistance to Ketones | low | |
Chemical Resistance to Maximum Concentrated Alkalis (at 50°C) | none | |
Chemical Resistance to Medium-High Concentrated Acids (at 50°C) | none | |
Chemical Resistance to Mineral Oils and Aliphatic Hydrocarbons | high | |
Compression set at 100°C | medium | |
Impermeability at gas (Oxygen and Nitrogen) | medium | |
Resistance to Flame | none | |
Resistance to Heat Aging | medium | |
Resistance to Low Temperatures | low | |
Resistance to Ozone and Weathering | high | |
Tear Strength | high |