Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 113 (DMO) Delicate Machinery Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 171B (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 327A (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 757SSG (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 774VH (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 774VHF (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 774VHF-MS (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 774VH-MS (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 875MS (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 875MS-UV (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants PG-2S Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants PG-3S Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants PG-8S Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | T10 |
Precision Polymer Engineering N60R Nitrile Rubber Red Nitrile Butadiene / PVC elastomer blend 59-65°IRHD. Electrically non-conductive. Copolymer of acrylonitrile and butadiene, blended with polyvinyl chloride.Applications: Specially formulated as .. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Temperature at which stiffness does not exceed 70 Mpa |
Precision Polymer Engineering N90M Nitrile Rubber Nitrile Rubber, 85-95 °IRHD. Meets British Standard BS2751 BA90. Medium acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR.Applica.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | |
Precision Polymer Engineering Perlast® G90A Perfluoroelastomer A black general purpose perfluoroelastomer compound with exceptionally high chemical resistance and excellent steam resistance and mechanical properties. Extremely low outgassing properties.Applicat.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | |
Precision Polymer Engineering V60F Fluoroelastomer Compound Peroxide/Litharge cured, Fluoroelastomer Rubber, 55-65 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line c.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | |
Precision Polymer Engineering V70A Fluoroelastomer Compound Blue Fluoroelastomer Rubber, 65-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK710, A1-10, B38, EF31, EO78, F15, Z1, Z2, where Z1 = comp-.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 875MS-G0 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 875R (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | |
Freudenberg Simrit V175 Aflasâ„¢ (TFE/P) Excellent resistance to acids, bases, water and amines. Widely used in oil fields. Avoid polar solvents and aromatic fuels. Compression set performance may be too high for some applications. Typical.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Continuous; DIN 52612 |
Isoflon PP Polypropylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | TR test, TR70 |
Daikin DAI-EL G-671 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 67% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Excellent low-temperature sealing .. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Gehman torsion test, T2 |
Daikin DAI-EL G-801 Fluoroelastomer Copolymer, Peroxide Curable Grade, 66% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good low-temperature and elasticity characteristics.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | ASTM D 3575 |
Eurofoam Evacell EVA 100 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | ASTM D 3575 |
Eurofoam Evacell EVA 200 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Service |
3M 3000WT Fire Barrier Water Tight Sealant 3M Fire Barrier Water Tight Sealant 3000 WT is a high-performance, ready-to-use, single component, neutral cure, non-slumping intumescent silicone sealant. Product cures upon exposure to atmospheric.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Application |
3M 8087 Construction Seaming Tape 3M™ Construction Seaming Tape 8087 is designed to seal seams on housewrap and insulated sheathing products. It can also be used to seam polyethylene vapor barrier products as well as to repair hole.. |