Thermal Properties Metric English Comments
Crystallization Temperature 133 °C
271 °F
Melting; DSC
LG Chemical LUTENE-H FE0070 HDPE
LUTENE-H FE0070 is mainly intended for the extrusion of blown film with high mechanical properties for the manufacture of "T-Shirt" grocery sacks, can liners. Especially, LUTENE-H FE0070 resin can b..
Crystallization Temperature 133 °C
271 °F
Melting; DSC
LG Chemical SEETEC PB150 HDPE
Features: This high molecular weight, hexane copolymer is tailored for high impact blow-molded containers that require:Excellent processabilityHigh impact strength at low temperatureOutstanding stre..
Crystallization Temperature 133 - 140 °C
271 - 284 °F
Peak; ASTM D3418
Solvay Specialty Polymers Ajediumâ„¢ PVDF 9009 Polyvinylidene Fluoride (PVDF)
Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea..
Crystallization Temperature 133 - 138 °C
271 - 280 °F
Peak; ASTM D3418
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran..
Crystallization Temperature 133 - 140 °C
271 - 284 °F
Peak; ASTM D3418
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53...
Crystallization Temperature 133 - 138 °C
271 - 280 °F
Peak, DSC; ASTM D3418
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Crystallization Temperature 133 - 140 °C
271 - 284 °F
Peak, DSC; ASTM D3418
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Crystallization Temperature 133 - 140 °C
271 - 284 °F
Peak, DSC; ASTM D3418
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)  (discontinued **)
Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Crystallization Temperature 133 °C
271 °F
Melting; DSC
LG Chemical LUTENE-H ME9180 HDPE
Description: LUTENE-H ME9180 is mainly intended for injection molding of complicated parts. It has high productivity and good appearance.Applications: Complicated parts, light-weight household.CAS N..