Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 113 °C | 235 °F | ASTM D3418 |
ExxonMobil HD 6510 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |
|||
Crystallization Temperature | 113 °C | 235 °F | ASTM D3418 |
ExxonMobil HD 6510.17 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |
|||
Crystallization Temperature | 113 °C | 235 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M10 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High stiffnessGood processingFair impact resistanceTypical Applications: General-purpose products, such as small-to-medium .. |
|||
Crystallization Temperature | 113 °C | 235 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M3804 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:High stiffnessGood processingFair impact resistanceTypical Applications: General-purpose products, such as small-to-medium wa.. |
|||
Crystallization Temperature | 113 °C | 235 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M90 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High stiffness and toughnessGood ESCRFair processingTypical Applications: Large, thick-wall parts, high-load products, such.. |
|||
Crystallization Temperature | 113 °C | 235 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M9001 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:High stiffness and toughnessGood ESCRFair processingTypical Applications: Large, thick-wall parts, high-load products, such a.. |
|||
Crystallization Temperature | 113 °C | 235 °F | ASTM D-3418 |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |
|||
Crystallization Temperature | 113 °C | 235 °F | ASTM D-3418 |
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren.. |
|||
Crystallization Temperature | 113 °C | 235 °F | ASTM D-3418 |
Chevron Phillips Marlex® HMN TR-945/945G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationGood impact stren.. |
|||
Crystallization Temperature | 113 °C | 235 °F | Equate Test Method |
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin EPDA-5040 is a high molecular weight high density polyethylene copolymer resin designed for non-pressure gravity pipe applications. It has a good balance of flexibility, ductility, stiffness and tou.. |
|||
Crystallization Temperature | 113 °C | 235 °F | Dow Method (DSC) |
Dow DNDA-1081 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1081 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Crystallization Temperature | 113 °C | 235 °F | Dow Method (DSC) |
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Crystallization Temperature | 113 °C | 235 °F | Dow Method (DSC) |
Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1149 NT 7 is produced using UNIPOL™ PE process technology and is intended for high-speed injection molding applications. Information provided by Dow |
|||
Crystallization Temperature | 113 - 115 °C | 235 - 239 °F | |
Addcomp PRIEX® 20095 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Crystallization Temperature | 113 °C | 235 °F | |
Addcomp PRIEX® Ionomer 33101 HDPE Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |
|||
Crystallization Temperature | 113 - 115 °C | 235 - 239 °F | |
Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Crystallization Temperature | 113 - 115 °C | 235 - 239 °F | ISO 11357-3 |
Addcomp PRIEX® 20097 Maleic Anhydride Grafted PP homopolymer Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fibre, wood flour, natural fibres, multilayer films, aluminium foils, .. |
|||
Crystallization Temperature | 113 °C | 235 °F | |
Addcomp PRIEX® Ionomer 30101 HDPE Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |