Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 247 °C | 477 °F | B |
Plastcom SLOVAMID 6 GF 20 GB 10 PA6, 20% glass fibre, 10% glass beads FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre and 10% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri.. |
|||
Vicat Softening Point | 247 °C | 477 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
Vicat Softening Point | 247 °C | 477 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Asia Pacific) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
Vicat Softening Point | 247 °C | 477 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
Vicat Softening Point | 247 °C | 477 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics EXTEM XH1015F TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1015 Resin. EFSA food Contact approved. |
|||
Vicat Softening Point | 247 °C | 477 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications. |
|||
Vicat Softening Point | 247 °C | 477 °F | B/120; ISO 306 |
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 247 °C | 477 °F | B/50; ISO 306 |
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 247 °C | 477 °F | 50°C/h 50N; ISO 306 |
LATI LATILUB 80-40GRT Polyphenylene sulfide Base (PPS), 40% Graphite and PTFE Self Lubricating Plastic
(U Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |