Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 190 °C | 374 °F | B |
Plastcom SLOVAMID 66 HI/1 TS PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PA (Europe-Africa-Middle East) NORYL GTX918W is an unfilled global grade, which offers an excellent combination of processability and heat resistance. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Asia Pacific) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
Vicat Softening Point | 190 °C | 374 °F | ASTM D1525 |
Toyobo PELPRENE™ P150B-05 Polyester TPE, Non-smell, Non-deposit Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo. |
|||
Vicat Softening Point | 190 °C | 374 °F | B/120; ISO 306 |
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 190 °C | 374 °F | 50N; ISO 306 |
Eurotec® Tecodur® PB70 KK45 NL XA 20 PBT 45% glass fiber/mineral reinforced, UL94 V0, low warpage Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Vicat Softening Point | 190 °C @Load 5.10 kg |
374 °F @Load 11.2 lb |
dry; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 MCS 850 Polyamide 6 - Flame Retarded, Unreinforced Glow wire resistance 850°C, bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has .. |
|||
Vicat Softening Point | 190 °C @Load 5.10 kg |
374 °F @Load 11.2 lb |
ISO 306 |
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac.. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Europe-Africa-Middle East) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Vicat Softening Point | 190 °C | 374 °F | 50 °C/h 10N; ISO 306 |
DSM Arnitel® CM622 TPC-ES 60 Shore D, Extrusion |