Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 156 °C | 313 °F | ASTM D1525 |
Multibase Nylex™ 2185 HF Polyamide + PP Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Vicat Softening Point | 156 °C | 313 °F | B |
Plastcom SLOVALEN PH 49 GF 10 GB 20 PP, 20% glass beads, 10% glass fibre, coupling agent FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10 % glass fiber and 20% glass beads, contains themodifier of mechanical properties. Increased strength in comparis.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Vicat Softening Point | 156 °C @Load 1.00 kg |
313 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CIP16020FCS Polypropylene, Fast Cycle Information provided by Polykemi AB |
|||
Vicat Softening Point | 156 °C | 313 °F | 50°C/h 50N; ISO 306 |
LATI LATAN 13 G/303 30% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Vicat Softening Point | 156 °C | 313 °F | 50°C/h 50N |
Covestro Apec® 1605 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation pr.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ASTM D1525-97 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ASTM D1525-97 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ASTM D1525-97 |
Ipiranga Petrochem PH 0321 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 156 °C @Load 1.02 kg |
313 °F @Load 2.25 lb |
GOST 15088 |
Sibur H250 GP Polypropylene Homopolymer Polypropylene homopolymer with narrow molecular weight distribution. It features high fluidity, an optimal stabilization package and balanced physical and mechanical properties.general purpose produ.. |
|||
Vicat Softening Point | 156 °C | 313 °F | |
Styron CALIBRE™ 200 10 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Vicat Softening Point | 156 °C | 313 °F | |
Styron CALIBRE™ 2060 10 Polycarbonate, Sterilization Grade CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clari.. |
|||
Vicat Softening Point | 156 °C @Load 5.10 kg |
313 °F @Load 11.2 lb |
Rate A (50°C/h); ASTM D1525 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, .. |
|||
Vicat Softening Point | 156 °C | 313 °F | |
Styron CALIBRE™ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
Vicat Softening Point | 156 °C | 313 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Vicat Softening Point | 156 °C | 313 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Vicat Softening Point | 156 °C | 313 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Vicat Softening Point | 156 °C | 313 °F | A (10N); ISO 306 |
Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength.. |
|||
Vicat Softening Point | 156 °C | 313 °F | B50 (50°C/h 50N); ISO 306 |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Vicat Softening Point | 156 °C @Load 1.02 kg |
313 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem PH 0130 HOMO Polypropylene Homopolymer PH 0130 is a low melt flow rate homopolymer with a general purpose additive package. This resin is designed for blow molding and extrusion. PH 0130 features excellent processability and stiffness/im.. |
|||
Vicat Softening Point | 156 °C | 313 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 300 GB6 POM 30% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Vicat Softening Point | 156 °C | 313 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 300 M POM Tribological modified grade with addition of molybdenum disulphide, which causes decreased coefficient of friction and wear, especially for applications requiring high load at low sliding speed.Info.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR6325 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 156 °C | 313 °F | 10 N; ASTM D1525 |
Braskem H 103 Extrusion Coating Polypropylene Homopolymer Description: H 103 is a high melt flow rate additivated homopolymer used for general purposes. The product exhibits excellent processing performance on injection moulding applications. Applications:.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ISO 306 |
Unipetrol PP MONSTEN® GB 107 Polypropylene Homopolymer Made for injection molding. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 156 °C | 313 °F | ISO 306 |
Unipetrol PP MONSTEN® GB 218 Polypropylene Homopolymer Applications include injection molding and fibers. Anti Gasfading stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 156 °C @Load 1.02 kg |
313 °F @Load 2.25 lb |
A50; ISO 306 |
Borealis Bormod™ HC904CF Polypropylene Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech.. |