Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 153 °C | 307 °F | ASTM D1525B |
SABIC PP 510P Polypropylene Homopolymer for Fiber Applications Product Description: PP 510P is a homopolymer specially designed for fiber extrusion applications with the following features:Consistent processabilityGood thread line stabilityGood color consisten.. |
|||
Vicat Softening Point | 153 °C | 307 °F | ASTM D1525B |
SABIC PP 575P Polypropylene Homopolymer for Injection Molding Product Description: PP 575P is specially developed for producing rigid injection molding articles for general purpose applications. It gives consistent processability and high gloss in the produc.. |
|||
Vicat Softening Point | 153 °C | 307 °F | ASTM D1525B |
SABIC PP 578P Polypropylene Homopolymer for Injection Molding Product Description: PP 578P is a controlled rheology PP grade of medium molecular weight distribution suitable for injection molding applications. It gives consistent processability, good flow pr.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® 243R PC (Europe-Africa-Middle East) LEXAN 243R is a medium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® AD143 PC LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® AD143 PC (Europe-Africa-Middle East) LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® AD4820 PC (Europe-Africa-Middle East) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® HP3AEU PC (Europe-Africa-Middle East) Lexan HP3AEU resin is a medium flow polycarbonate with mold release designed for medical devices and pharmaceutical applications. It is assessed with biocompatible ISO10993 (or USP Class VI) and is.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® HP4R PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a hig.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East) LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® 143 PC (Europe-Africa-Middle East) LEXAN 143 is a medium viscosity U.V. stabilized multi purpose grade. LEXAN 143 is available in transparent, translucent and opaque colours. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® HP4 PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Vicat Softening Point | 153 °C @Load 1.00 kg |
307 °F @Load 2.20 lb |
ASTM D1525 |
LG Chemical SEETEC H1501 Polypropylene Homopolymer Features: SEETEC H1501 is a homopolymer for injection molding. H1501 is specifically developed for application demanding a high stiffness and a high fluidity. SEETEC H1501 meets the FDA requirement .. |
|||
Vicat Softening Point | 153 °C | 307 °F | A120; ISO 306 |
Inno-Comp INNOPOL® CS 1-5120 BLH 20% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-5120 BLH is a 20% talc-filled polypropylene homopolymer compound /PP-H TD20 (ISO 1043)/.INNOPOL® CS 1-5120 BLH is recommended especially for producing products, where high stiffn.. |
|||
Vicat Softening Point | 153 °C | 307 °F | ASTM D1525-97 |
Ipiranga Petrochem PH 1721 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 153 °C | 307 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
Vicat Softening Point | 153 °C | 307 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® GN-3430R Improved Mold Release, Glass Fiber Reinforced, Flame Resistant Polycarbonate Resin GF 30% reinforced, flame retardant and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machin.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Loading 1 (10N); ASTM D1525 |
Teknor Apex Sinpolene TPP1010 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Housings Forms: Pellets Processing Method: Injection Mol.. |
|||
Vicat Softening Point | 153 °C | 307 °F | 10N-50°C per hour; ISO 306 |
Total PPH 9069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9069 is homopolymer.ApplicationATOFINA Polypropylene PPH 9069 is intended for applications in non-wovens. It is also suitable for extrusion of bulk continuous filament (BC.. |
|||
Vicat Softening Point | 153 °C | 307 °F | -1kg; ASTM D1525 |
Braskem H 107 Coating Polypropylene Description: H 107 is a ultra-high melt flow rate additivated homopolymer used for general purposes. Designed for extrusion coating. This product exhibits excellent processability, good melt stabili.. |
|||
Vicat Softening Point | 153 °C @Load 1.02 kg |
307 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem PH 1721 HOMO Polypropylene Homopolymer PH 1721 is a low melt flow rate polypropylene with an anti-gas fading stabilization package. It is suitable for continuous filament and staple fiber processing due to its molecular weight distributi.. |
|||
Vicat Softening Point | 153 °C | 307 °F | ISO 306/A50 |
Addiplast Addilene H 490 S Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Vicat Softening Point | 153 °C | 307 °F | ISO 306/A50 |
Addiplast Addilene H 530 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Vicat Softening Point | 153 °C | 307 °F | ISO 306/A50 |
Addiplast Addilene H 532 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Vicat Softening Point | 153 °C | 307 °F | ISO 306/A50 |
Addiplast Addilene H 560 Polypropylene Homopolymer High heat resistance, detergent stabilized, anti-yellowingInformation provided by Addiplast. |
|||
Vicat Softening Point | 153 °C | 307 °F | ISO 306/A50 |
Addiplast Addilene PMD 50245 Polypropylene Homopolymer For electroplatingInformation provided by Addiplast. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FXG154 PC (Asia Pacific) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML144R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc.. |
|||
Vicat Softening Point | 153 °C @Load 1.02 kg |
307 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem CP 404XP HECO Polypropylene Heterophasic Copolymer CP 404XP is a medium melt flow rate heterophasic copolymer with suitable additives to produce caps and closures for carbonated beverages. This product exhibits high stiffness and impact strength bal.. |