Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1200 is a PC+ABS blend developed to serve extremely demanding applications in a variety of markets while maintaining good processing properties. The combination of superior heat resistance .. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Asia Pacific) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FXE4271L PC (Asia Pacific) Lexan* FXE4271L is a 10% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1200HF is the improved version of CYCOLOY C1200 and has been developed to provide enhanced productivity and surface appearance for |
|||
Vicat Softening Point | 132 °C | 270 °F | ASTM D1525 |
Ineos A60-70-162 HDPE Ineos A60-70-162 is a high density polyethylene homopolymer, developed specifically for blow molding food containers on reciprocating screw-type equipment. It exhibits excellent processing character.. |
|||
Vicat Softening Point | 132 °C | 270 °F | ASTM D1525 |
Ineos K50-10-136 HDPE Ineos K50-10-136 is a high molecular weight, high density polyethylene copolymer. This product was developed for blowmolding automotive fuel tanks and other large parts, where the finished produc.. |
|||
Vicat Softening Point | 132 °C | 270 °F | ASTM D1525 |
Ineos K54-05 HDPE K54-05 is a high molecular weight, high density polyethylene copolymer developed for large-part blow molding (drum market) where the finished product demands outstanding physical performance. This m.. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X6125 PBT+PC Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Europe-Africa-Middle East) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Europe-Africa-Middle East) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Xylex X7503HP PC+POLYESTER (Europe-Africa-Middle East) Clear PC-Siloxane copolymer + Polyester alloy, USA Food ContactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Asia Pacific) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Vicat Softening Point | 132 °C | 270 °F | ISO 306 |
Unipetrol PP MONSTEN® GB 802 Polypropylene Random Copolymer Applications include injection molding and extrusion. Basic stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 132 °C | 270 °F | ISO 306 |
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Vicat Softening Point | 132 °C | 270 °F | ISO 306 |
Total HDPE HL 717 High Density Polyethylene - Blown Film HDPE HL 717 is a high density polyethylene produced by the gas phase polymerization process with hexene as a comonomer.HDPE HL 717 is a monomodal HDPE with a broad molecular weight distribution. It.. |
|||
Vicat Softening Point | 132 °C | 270 °F | A/50 (10 N); ISO 306 |
Borealis Daploy™ SF203HMS High Melt Strength Polypropylene for Extrusion Coating Daploy SF203HMS resin is a statistic-heterophasic-propylene-ethylene copolymer modified with a polypropylene based structurally isomeric polymer which combines a significantly increased melt strengt.. |
|||
Vicat Softening Point | 132 °C @Load 1.02 kg |
270 °F @Load 2.25 lb |
A50; ISO 306 |
Borealis RD735CF Polypropylene Random Copolymer RD735CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD735CF is recommended for food packaging, textile packaging .. |
|||
Vicat Softening Point | 132 °C | 270 °F | ISO 306 |
Unipetrol PP MONSTEN® MT 812 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 132 °C @Load 5.00 kg |
270 °F @Load 11.0 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND PSA 7600 PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 132 °C | 270 °F | |
Covestro Bayblend® T 88-4N Polycarbonate/ABS Blend, 20% Glass Fiber Contains 20% glass fiber reinforcement, high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – .. |
|||
Vicat Softening Point | 132 °C | 270 °F | 50°C/h 50N; ISO 306 |
Covestro Bayblend® T88 GF-10* Polycarbonate + SAN Glass Filled Impact Grade Developmental productInjection molding grade10 % GFoptimized heat ageing- and UV-stabilityvery good flowtensile modulus = 5100 MPaVicat/B 120 = 134 °CPreprocessingMax. Water content |
|||
Vicat Softening Point | 132 °C | 270 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ABS TM 40 Description: Heat Resistant Grade, Ultra High HeatInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 132 °C | 270 °F | 50°C/hr; 50N |
Arkema Group Pebax® 4033 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Vicat Softening Point | 132 °C | 270 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Vicat Softening Point | 132 °C @Load 1.02 kg |
270 °F @Load 2.25 lb |
A50; ISO 306 |
Borealis WG341C Polypropylene WG341C is a polypropylene for extrusion coating. Applications: microwave oven applications, extrusion coating of high volume production of boards and papers, coating of textile fibers, pinholes fre.. |