Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 119 °C @Load 1.00 kg |
246 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Eraclene® FB 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FB 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
NOVA Chemicals Sclair® 15A Butene HDPE Film Resin Film Properties. Features: Low gel, good barrier properties, strength and toughness.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2714 HDPE Injection Molding Resin Features: Excellent processability for applications requiring good stiffness and toughness, good cold temperature impact properties.Applications: Food containers and lids, frozen food containers.Dat.. |
|||
Vicat Softening Point | 119 °C | 246 °F | 50°C/hr; 50N |
Polimeri Europa KOBLEND HI PD 19 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend with a very good impact behaviour, good stiffness and higher thermal properties than KOBLEND HI 18. Main application field.. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
SABIC R40039E Medium Density Polyethylene for Rotational Molding Product Description: R40039E is a Medium Density Polyethylene grade designed to provide excellent mechanical properties with high rigidity, toughness, gloss and low warpage. R40039E is UV stabiliz.. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
NOVA Chemicals Novapol® HD-2100-A MDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
NOVA Chemicals Sclair® 14K1 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
NOVA Chemicals Sclair® 14K3 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2508-UV9 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids.Data provided by the manufacturer. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
LyondellBasell Petrothene® LP540200 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP540200 is a copolymer resin designed for blown film applications. This resin offers high ESCR, stiffness, excellent appearance and bubble stability. LP540200 is recommended for high str.. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
Mitsui ADMER® QF551A PP Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Vicat Softening Point | 119 °C | 246 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Vicat Softening Point | 119 °C | 246 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 119 °C | 246 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 119 °C | 246 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 119 °C | 246 °F | 120°C/hr, 1kg; ISO 306-A |
Styron Magnumâ„¢ 3416 SC Natural Plus ABS Resin The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent processability with sable light base color that is ideal for self-coloring.Information provided by Do.. |
|||
Vicat Softening Point | 119 °C | 246 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Vicat Softening Point | 119 °C | 246 °F | ISO 306 |
Unipetrol PE HD LITEN® PL 10 HDPE Pipe applications.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 119 °C | 246 °F | ISO 306 |
Total Lumicene® mPE M 2704 EP S01 Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M 2704 EP S01 is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2704 EP S01 can be.. |
|||
Vicat Softening Point | 119 °C | 246 °F | |
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food .. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
Dow DOWLEX™ 2036G Linear Low Density Polyethylene Improved thermal stability for high stiffness film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Vicat Softening Point | 119 °C | 246 °F | |
Dow DOWLEX™ IP-22 High Density Polyethylene DOWLEX® IP-22 resin is an improved processing high density polyethylene resin designed for excellent flow, high impact, and moderate stiffness. DOWLEX IP-22 resin balances peak molecular weight wit.. |
|||
Vicat Softening Point | 119 °C @Load 1.00 kg |
246 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Vicat Softening Point | 119 - 152 °C | 246 - 306 °F | Average value: 136 °C Grade Count:6 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Vicat Softening Point | 119 °C | 246 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2508-UV13 MDPE Injection Molding Resin
(discontinued **) Excellent processability for applications requiring stiffness and toughness, Good cold temperature impact propertiesApplications: Roll-out cart lidsAdditives: Elevated levels of ultraviolet light st.. |