Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 95.6 °C | 204 °F | ASTM D1525-B |
Americas Styrenics STYRON™ A-TECH™ 6079 Ignition Resistant Polystyrene Resin
(discontinued **) STYRON™ A-TECH™ 6079 is an ignition resistant polystyrene (IRPS) resin designed specifically for consumer and business electronics applications that demand excellent aesthetics, along with a stron.. |
|||
Vicat Softening Point | 95.6 °C | 204 °F | ASTM D1525 |
M. Holland Company GS410WC Polystyrene
(discontinued **) Features: High Clarity, High FlowUses: Household Goods, LabwareApprovals: FDA 21 CFR 177.1640 Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Vicat Softening Point | 95.6 °C | 204 °F | ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PE3-0200RX Biocompatible LDPE A biocompatible Low Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Vicat Softening Point | 95.6 °C | 204 °F | ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PE3-0202AF Food Grade LDPE Low Density Polyethylene with FDA food contact approval and antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Vicat Softening Point | 95.6 °C | 204 °F | ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PE3-0202ARX Biocompatible, Antimicrobial LDPE A biocompatible Low Density Polyethylene for healthcare applications containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Vicat Softening Point | 95.6 °C | 204 °F | ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PE3-0205ARX Biocompatible, Antimicrobial LDPE A biocompatible Low Density Polyethylene for healthcare applications containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Color Compo.. |
|||
Vicat Softening Point | 95.6 °C | 204 °F | ASTM D1525 |
Total PSI 945 Polystyrene Polystyrene 945 is designed for injection molding applications requiring superior toughness. This polymer is a high impact polystyrene with excellent gloss and falling dart properties. The impact an.. |
|||
Vicat Softening Point | 95.6 °C | 204 °F | ASTM D1525 |
American Polymers API 645-21 Polystyrene API 645-21 is a super high impact polystyrene used in applications requiring a superior level of toughness along with good tensile and flexural properties. On balance this extrusion grade polymer a.. |
|||
Vicat Softening Point | 95.6 °C | 204 °F | ASTM D648 |
LTL Color Compounds ColorRx™ PE3-0201A Antimicrobial LDPE Low Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders, Inc. |
|||
Vicat Softening Point | 95.6 °C | 204 °F | |
Styron Magnum™ 4435 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |