LTL Color Compounds ColorRxâ„¢ PE3-0202AF Food Grade LDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer LTL Color Compounds
Trade Name ColorRx™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LTL Color Compounds ColorRxâ„¢ PE3-0202AF Food Grade LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low Density Polyethylene with FDA food contact approval and antimicrobial protection.All information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.5 MPa
2100 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 1.79 GPa
260 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 95.6 °C
204 °F
ASTM D648