Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Americas Styrenics STYRON™ A-TECH™ 6079 Ignition Resistant Polystyrene Resin  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Americas Styrenics STYRON™ A-TECH™ 6079 Ignition Resistant Polystyrene Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
STYRON™ A-TECH™ 6079 is an ignition resistant polystyrene (IRPS) resin designed specifically for consumer and business electronics applications that demand excellent aesthetics, along with a strong blend of toughness and flow/process-ability characteristics. Its high melt flow enables faster cycle times and better flow molding, which reduces scrap/waste. In addition, the molder has a wider operating window with the parameters for larger tools. Available in five colors: Natural, Light Gray, Gray #5, Gray, and Black. Applications Consumer electronics: larger size TV cabinets Large and/or hard-to-fill parts (including no-paint) Small portable electronics: cellular phones, pagers, etc. Information technology/business equipment: hard drives, monitors, keyboards, printers, fax machine housing, etc. Information provided by DowAmericas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formation.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 200 °C
12 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 16.1 MPa
2340 psi
Injection molded; ASTM D638
Tensile Strength, Yield 17.9 MPa
2600 psi
Injection molded; ASTM D638
Elongation at Break 46 %
46 %
Injection molded; ASTM D638
Tensile Modulus 2.07 GPa
300 ksi
Injection molded; ASTM D638
Flexural Strength 37.0 MPa
5360 psi
Injection molded; ASTM D790
Flexural Modulus 2.09 GPa
303 ksi
Injection molded; ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
Injection molded; ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 95.6 °C
204 °F
ASTM D1525-B
Flammability, UL94 V-0
V-0
0.0625 in. thickness
Users viewing this material also viewed the following: