Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 84.4 °C | 184 °F | ASTM D1525 |
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade ApplicationsMicrothene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh pow.. |
|||
Vicat Softening Point | 84.3 °C | 184 °F | Phr = 8 |
Shandong Rike Chemical HELIâ„¢ HL-57 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Vicat Softening Point | 84.6 °C @Load 5.00 kg |
184 °F @Load 11.0 lb |
|
Shandong Rike Chemical HELIâ„¢ HL-740 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Vicat Softening Point | 84.5 °C @Load 5.00 kg |
184 °F @Load 11.0 lb |
|
Shandong Rike Chemical HELIâ„¢ HL-766 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Vicat Softening Point | 84.7 °C @Load 5.00 kg |
184 °F @Load 11.0 lb |
|
Shandong Rike Chemical HELIâ„¢ HL-769 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Vicat Softening Point | 84.6 °C | 184 °F | Phr = 8 |
Shandong Rike Chemical HELIâ„¢ HL-2005 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Vicat Softening Point | 84.4 °C | 184 °F | ASTM D1525 |
ExxonMobil LD 307.76 Clear, High Impact Film Resin LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical |