Download PDF Shandong Rike Chemical HELIâ„¢ HL-740 Weather-resistance Acrylic Impact Modifier (AIM).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic copolymers. The basic functions of our impact modifiers are to improve the impact performance of PVC products to meet the requirements of engineering plastics and simultaneously increase their heat and light stability.Information Provided by Shandong Rike Chemical Co., Ltd.
Physical Properties Metric English Comments
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
Volatiles <= 1.0 %
<= 1.0 %
Particle Mesh Size 30 Mesh
30 Mesh
<2%
Mechanical Properties Metric English Comments
Tensile Strength 46.7 MPa

@Temperature 18.0 °C,
Time 86400 sec
6770 psi

@Temperature 64.4 °F,
Time 24.0 hour
Izod Impact, Unnotched (ISO) 27.9 kJ/m²

@Temperature 0.000 °C,
Time 86400 sec
13.3 ft-lb/in²

@Temperature 32.0 °F,
Time 24.0 hour
Thermal Properties Metric English Comments
Vicat Softening Point 84.6 °C

@Load 5.00 kg
184 °F

@Load 11.0 lb
Descriptive Properties Value Comments
Appearance White powder