Shandong Rike Chemical HELIâ„¢ HL-2005 Weather-resistance Acrylic Impact Modifier (AIM)

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Shandong Rike Chemical
Trade Name HELI™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Rike Chemical HELIâ„¢ HL-2005 Weather-resistance Acrylic Impact Modifier (AIM).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic copolymers. The basic functions of our impact modifiers are to improve the impact performance of PVC products to meet the requirements of engineering plastics and simultaneously increase their heat and light stability.Information Provided by Shandong Rike Chemical Co., Ltd.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 14.6 kJ/m²

@Temperature 0.000 °C
6.95 ft-lb/in²

@Temperature 32.0 °F
Phr = 0
19.1 kJ/m²

@Temperature 0.000 °C
9.09 ft-lb/in²

@Temperature 32.0 °F
Phr = 5
19.7 kJ/m²

@Temperature 23.0 °C
9.37 ft-lb/in²

@Temperature 73.4 °F
Phr = 0
25.3 kJ/m²

@Temperature 0.000 °C
12.0 ft-lb/in²

@Temperature 32.0 °F
Phr = 8
34.7 kJ/m²

@Temperature 23.0 °C
16.5 ft-lb/in²

@Temperature 73.4 °F
Phr = 5
37.1 kJ/m²

@Temperature 23.0 °C
17.7 ft-lb/in²

@Temperature 73.4 °F
Phr = 8
Thermal Properties Metric English Comments
Vicat Softening Point 84.6 °C
184 °F
Phr = 8
86.0 °C
187 °F
Phr = 0
Descriptive Properties Value Comments
Light Aging - Whiteness Variation (%) 15.3
Phr = 8
17.1
Phr = 5
51.22
Phr = 0
Thermal Aging - Whiteness Variation (%) 20.4
Phr = 0
26.8
Phr = 5
31.1
Phr = 8