Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D 1525 |
NOVA Chemicals Novapol® LF-0718-A-INJECTION LDPE Injection Molding Resin LF-0718-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. LF-0718-A is subj.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D1525 |
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D1525 |
Petroquimica Triunfo Trithene® JX 7065 LDPE - Injection Molding and Master Batch The Trithene® JX 7065 resin is a low-density polyethylene with a wide molecular weight distribution, developed to offer good impact resistance, excellent flexibility, and high resistance to stress .. |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ASTM D1525 |
Global ST-1018 Low Density Polyethylene, Injection Molding Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.15.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D1525 |
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 83.0 - 85.0 °C @Load 5.00 kg |
181 - 185 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 520/1 Rigid PVC, Extrusion Electric pipes |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D1525 |
LyondellBasell Microthene® G MN71020 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D1525 |
LyondellBasell Microthene® G MN71120 Low Density Polyethylene (Rotomolding) General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ISO |
I. Stern N1921 General Purpose Crystal Polystyrene Features:Excellent ProcessabilityEasy FlowApplicationsDisposable PackagingHousewaresCosmetics PackagingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. Stern & Co. In.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | VST/B/50; ISO 306 |
GEHR Plastics PE-ELS® Polyethylene HDPE A variant of PE-HD with improved electrical conductivity.Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties a.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | |
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 210E is most commonly used for thermoformed sheet applications. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D1525 |
Mitsui ADMER® NF548A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ISO 306 |
Stir SpA RI 1 A (PVC) Application: Spiral extrusion, shock resistantInformation provided by STIR SpA |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ASTM D1525 |
Teknor Apex Sinvicomp SBB 3700 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Medium Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provi.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D1525 |
DuPont Bynel® 4206 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D648 |
Wanshijie PETG Sheet PETG is also named GPET. It is made of a kind of non-crystalline PET resin sourced from cyclohexanediol modification. PETG differs greatly from PET and PCT. PETG is a kind of non-crystalline copolym.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | 1kg load; ASTM D1525 |
Eastman Spectar® 14471 Copolyester Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use .. |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ASTM D1525 |
ExxonMobil LD 306.38 High Clarity, High Impact Film Resin LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ASTM D1525 |
ExxonMobil LD 306.57 High Clarity, High Impact Film Resin LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 83.0 - 85.0 °C @Load 5.00 kg |
181 - 185 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds R 220 Rigid PVC, Extrusion Rolling shutters |
|||
Vicat Softening Point | 83.0 - 85.0 °C @Load 5.00 kg |
181 - 185 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds R 220/R Rigid PVC, Extrusion Shiny rolling shutters |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ISO 306 |
Arkema Group OREVAC® 18370 Maleic Anhydride Modified Polyethylene OREVAC® 18370 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ISO 306 |
Arkema Group OREVAC® 18380 Maleic Anhydride Modified Polyethylene OREVAC® 18380 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Vicat Softening Point | 82.8 °C | 181 °F | 50°C/hr; 50N; ASTM D1525 |
Arkema Group Solarkote® PB Acrylic For PVC/acrylic alloys Information provided by Arkema Group |
|||
Vicat Softening Point | 83.0 °C | 181 °F | |
BASF Novolen® 2248 TC Polypropylene Nucleated grade with antistatic agent for injection moldings.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1020 VB 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding rigid articles. Examples: closures, ice trays.ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ASTM D1525 |
CPC - Vycom Ultra White™ PVC Advanced, UV (Ultra Violet) resistant sheet Ultra White is an advanced PVC formulation designed specifically for outdoor applications where resistance to ultraviolet (UV) degradation is critical. Tests show that Ultra White retards both surfa.. |
|||
Vicat Softening Point | 83.0 - 85.0 °C @Load 5.00 kg |
181 - 185 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 130 Rigid PVC, Extrusion Pipes and profiles |
|||
Vicat Softening Point | 83.0 °C | 181 °F | |
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |