Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 73.0 °C | 163 °F | ISO 306 |
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film Product Description: FI0644 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Vicat Softening Point | 73.0 °C @Load 1.00 kg |
163 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® FC 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FC 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FC 45 exhibit good optical properties, excellent impact resistance and low creep.. |
|||
Vicat Softening Point | 73.0 °C @Load 1.00 kg |
163 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 45 show high toughness.Main Applications: Greenflex FF 45 is recommended for.. |
|||
Vicat Softening Point | 73.0 - 85.0 °C | 163 - 185 °F | Average value: 79.2 °C Grade Count:5 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | |
Eastman Eastar GN101 PETG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Vicat Softening Point | 73.0 °C | 163 °F | Rate A; ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® CP 1315
(discontinued **) PRE-ELEC CP 1315 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525 |
LyondellBasell Ultrathene® UE635000 Ethylene Vinyl Acetate Copolymer, Extrusion Coating Grade ULTRATHENE UE635000 is an ethylene vinyl acetate copolymer recommended for extrusion coatings on cellophane, polypropylene and polyester. UE635000 is also used in special coextruded substrate coatin.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ISO 306 |
Manifattura Cattaneo PVC HI Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Vicat Softening Point | >= 72.8 °C | >= 163 °F | ASTM D 1525 |
Karina E 858-10/16-ERYA PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | 72.8 °C | 163 °F | ASTM D1525 |
Techmer ES HiFill® TPU 85A 0152 S1 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 865A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525 |
SK Chemicals SKYTHANE® T865A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525, ISO 306 |
DuPont Surlyn® 1650SB DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to .. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | A50; DIN 53460 |
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525 |
DuPont Elvax® 750 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | A50; DIN 53460 |
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525 |
DuPont™ Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1650 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525, ISO 306 |
DuPont™ Surlyn® 8528 Sodium Ionomer Surlyn® 8528 is a sodium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 8528 thermoplastic resi.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525 |
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU) A novel copolymer that is strong yet flexible with proven biocompatibility and biostability
Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | 50°C/hr; 50N |
Arkema Group Nakan® RRS 401 L PVC, Rigid Injection Grade NAKAN RRS 401 L is a rigid polyvinyl chloride compound developed for injection molding of waste water fittings.ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1003 VL 4S Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Grade for transparent and thermal agricultural film to 180 at 200 µ for greenhouse coverage.ISO data prov.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1003 VN 4 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for transparent and thermal agricultural film for greenhouse coverage.ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR8025 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525 |
Toyobo Pelprene™ P-30B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525, ISO 306 |
DuPont™ Surlyn® 1825 Zinc Ionomer Surlyn® 1825 is available for use in conventional blown, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1825 comp.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | B (50N); ISO 306 |
Borealis Xmod™ MC55T1 Polypropylene Compound 10% Mineral Filled Xmod MC55t1 is a 10% mineral filled grade based on HCPP intended for injection molding. Xmod has been developed especially for the car industry, to be used in interior parts. XMod offers very good .. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 9730 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9730 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Vicat Softening Point | 73.0 °C | 163 °F | ASTM D1525 |
DuPont Bynel® 20E482 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |