Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 63.0 °C @Load 1.00 kg |
145 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® ML 40 Ethylene Vinyl Acetate Copolymer - Injection Molding Greenflex ML 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding of flexible items. Items produced with Greenflex ML 40 show high elasticity and flexibility.Main Applications: Gr.. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-721 High EVA Coextrusion Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin providing outstanding heat sealability along with excellent strength, properties and clarity.App.. |
|||
Vicat Softening Point | 63.0 - 65.0 °C @Load 5.00 kg |
145 - 149 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RST 0413 Rigid PVC, Extrusion Lead Free Transparent antishock profiles |
|||
Vicat Softening Point | 63.0 °C | 145 °F | A; ISO 306 |
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | VST/B/50; ISO 306 |
Styrolution Styrolux® 656 C SBC Description: Styrolux® 656 C is a clear styrene-butadiene copolymer (SBC) with enhanced flow properties. It is used almost exclusively for injection molding of rigid, tough parts requiring highes.. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | B (50N); ISO 306 |
Borealis Daplen™ EE040AE TPO Compound Daplen EE040AE is an elastomer modified polypropylene compound intended for injection molding. Daplen EE040AE is a material with excellent impact /stiffness ratio. Thanks to its low thermal expansi.. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | A50; DIN 53460 |
Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | ASTM D1525 |
Chevron Phillips K-Resin® KR53 Styrene-Butadiene Copolymer Customer Benefits:Excellent ClarityHigh Surface GlossGood ToughnessGood Heat SealabilityTypical Applications:Medical PackagingProduce PackagingTwist WrapLidstock and Labeling FilmInformation provide.. |
|||
Vicat Softening Point | 62.8 °C | 145 °F | ASTM D1525 |
ExxonMobil Escorene® LD 713.93 Molding, extrusion and compounding resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer with very good toughness, high clarity and excellent processability. It is suitable for use in making molded articles, extruded profile.. |
|||
Vicat Softening Point | 62.8 °C | 145 °F | ASTM D1525 |
ExxonMobil Escorene™ UL 00514 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00514 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 250°C (482°F) may cause resin degradation.Availability: Africa & Mid.. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | ASTM D1525, ISO 306 |
DuPont™ Entira® ASSD100 Ionomer Resin DuPont™ Entira™ AS SD100 is an extremely hygroscopic ionomer resin that is supplied as free flowing pellets. Entira™ AS SD100 is used to lower the static decay time and surface resistivity of LD.. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 8940 Ionomer Resin, Sodium Surlyn® 8940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | B50 (50N); ISO 306 |
Domo 2448L Polypropylene Copolymer Information provided by Domo. |
|||
Vicat Softening Point | 62.8 °C | 145 °F | ASTM D1525 |
ExxonMobil Escorene™ LD 708.62 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 708.62 is a 14.9% VA copolymer film resin. Film made from LD 708.62 exhibits good impact strength and superior heat sealabilty.Availability: Latin America, Nor.. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR6518 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | |
BASF Novolen® 2448 L Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1020 VG 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high mechanical properties. Examples: films, chemical bags, gloves.ISO data provided by the manufactur.. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 7940 Ionomer Resin, Lithium Surlyn® 7940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne.. |
|||
Vicat Softening Point | 63.0 - 91.0 °C | 145 - 196 °F | Average value: 76.4 °C Grade Count:30 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Vicat Softening Point | 63.0 °C | 145 °F | A50; DIN 53460 |
Lubrizol ESTANE® 54620 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |