Lubrizol ESTANE® 54620 Ester Based Thermoplastic Polyurethane (European Grade)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 54620 Ester Based Thermoplastic Polyurethane (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.Benefits of Estane® TPU: Outstanding Abrasion and Wear ResistanceExcellent Low Temperature FlexibilitySuperior Toughness and DurabilityEase of Processing and Manufacturing FlexibilityColorability and Paintability with no adhesion promoterApplications: Film & SheetFabric coating & melt coatingWire & CableHose, Tube & ProfileCustom moldingCustom compoundingAutomotive interior/chassis and exterior painted trimInformation provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
DIN 53479
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
DIN 53505
Tensile Strength, Ultimate 33.0 MPa
4790 psi
DIN 53504
Elongation at Break 630 %
630 %
DIN 53504
50% Modulus 0.00460 GPa
0.667 ksi
DIN 53504
100% Modulus 0.00510 GPa
0.740 ksi
DIN 53504
300% Modulus 0.00790 GPa
1.15 ksi
DIN 53504
Tear Strength 70.0 kN/m
399 pli
DIN 53515
Abrasion 30
30
mm<sup>3</sup>; DIN 53516
Compression Set 25 %
25 %
70 hrs./22°C; DIN 53517
75 %
75 %
24 hrs./70°C; DIN 53517
Thermal Properties Metric English Comments
Vicat Softening Point 63.0 °C
145 °F
A50; DIN 53460
Brittleness Temperature -70.0 °C
-94.0 °F
DIN 53546