Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 55.0 °C @Load 1.00 kg |
131 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® CH D0 Very Low Density Polyethylene Clearflex CH D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The film has a high stretchability and an optimum cling effect.Main Applications:.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ISO 306/B50 |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | Vicat A, 1 kg; DIN 53460/ISO 306 |
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525 |
Westlake EMAC® SP2405 20% Ethylene-Methyl Acrylate Copolymer
(discontinued **) Westlake EMAC® SP2405 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperature are required. SP2405 provides.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-723 High EVA Extrusion Coating Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525 |
Huntsman IROGRAN® PS455-203 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Vicat Softening Point | 55.0 °C | 131 °F | (A50 (50°C/h 10 N)); ISO 306 |
LyondellBasell Adflexâ„¢ Q 100 F Polyolefin Description: Adflexâ„¢ Q 100 F is a thermoplastic polyolefin which has been developed for the extrusion of blown film, it is also suitable for sheet extrusion. Adflexâ„¢ Q 100 F features a ver.. |
|||
Vicat Softening Point | 55.0 °C @Load 5.00 kg |
131 °F @Load 11.0 lb |
|
LATI Latigea B01 I8 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |
|||
Vicat Softening Point | 55.0 °C | 131 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525 |
Westlake EBAC® Plus SP1903 18% Ethylene Butyl Acrylate Copolymer Westlake EBAC® SP1903 is an 18% EBA copolymer designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1903 provides excel.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525 |
Westlake EBAC® SP1806 17.5%, Ethylene-Methyl Acrylate Copolymer Description: Westlake EBAC® SP1806 is an ethylene butyl acrylate copolymer designed for extrusion coating and laminating. SP1806 can also be compounded as an impact modifier or used in highly fill.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525 |
Westlake EMAC® SP2205 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2205 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2205 provide.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D-1525 |
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane Features: Hard, flexible, abrasion resistant coatings. Primarily used for all solution binder for inks and lacquers on fabrics and various substrates.Uses: Adhesives and inks & lacquers, pigment bin.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525 |
ExxonMobil Escorene™ LD 723.28 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 723.28 is a 18.5 wt% vinyl acetate copolymer suitable for injection molding and compounding applications.Availability: Latin America, North America and South A.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525 |
ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 726.07 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. LD 716.07 is an excelle.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525 |
ExxonMobil EXACT™ 4049 Plastomer for Elastic Film and Elastic Film Blends Product Description: Exact 4049 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed for use as the cling component in mul.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525, ISO 306 |
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a .. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525, ISO 306 |
DuPont™ Elvax® 3155 Ethylene Vinyl Acetate DuPont™ Elvax® 3155 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 31.. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525 |
Arkema Group Orevac® 9304 Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Vicat Softening Point | 55.0 °C | 131 °F | |
BASF Procom® D 1146 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | |
BASF Procom® D 1158 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | |
BASF Procom® D 1165 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525 |
DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating 22.5 wt% Vinyl Acetate.Elvax® 3200-2 is an extrudable, wax-modified, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process .. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | Rate B; ASTM D-1525 |
ExxonMobil Iotek® 8030 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.Excellent abrasion resistance, impact strength, hardness, and tensile strength. Iotek ionomers provide superb low temperature impact strength when .. |
|||
Vicat Softening Point | 55.0 °C | 131 °F | ASTM D1525 |
DuPont Bynel® 2169 Anhydride-Modified Ethylene Acrylate Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |
|||
Vicat Softening Point | 55.0 - 160 °C | 131 - 320 °F | Average value: 111 °C Grade Count:6 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Vicat Softening Point | 55.0 °C @Load 5.00 kg |
131 °F @Load 11.0 lb |
|
LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |