Material Notes:
Product Description: Escorene Ultra LD 723.28 is a 18.5 wt% vinyl acetate copolymer suitable for injection molding and compounding applications.Availability: Latin America, North America and South America Additive:Anitblock: NoSlip: NoThermal Stabilizer: Yes Applications:CompoundingExtrusion CompoundsInjection MoldingMolding CompoundsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ExxonMobil method
Vinyl Acetate Content 18.5 %
18.5 %
ExxonMobil method
Melt Flow 23 g/10 min

@Load 2.16 kg,
Temperature 190 °C
23 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75

@Time 15.0 sec
75

@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 32

@Time 15.0 sec
32

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 7.58 MPa
1100 psi
ASTM D638
Tensile Strength, Yield 4.55 MPa
660 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Elongation at Yield 150 %
150 %
ASTM D638
Flexural Modulus, 1% Secant 51.7 MPa
7500 psi
ASTM D790
Dart Drop, Total Energy 13.6 J

@Temperature 22.8 °C
10.0 ft-lb

@Temperature 73.0 °F
ASTM D3763
24.4 J

@Temperature -40.0 °C
18.0 ft-lb

@Temperature -40.0 °F
ASTM D3763
Thermal Properties Metric English Comments
Melting Point <= 185 °C
<= 365 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 55.0 °C
131 °F