Material Notes:
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and neck-in and can be coextruded with homopolymer extrusion coating resins on most coextrusion coating lines.Applications: Heat seal layer for cheese packaging; Other extrusion coating applications requiring outstanding heat sealability.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
Exxon Method
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50, Condition A; ASTM D1693
Melt Flow 22.5 g/10 min
22.5 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
ASTM D2240
Hardness, Shore D 27
27
ASTM D2240
Tensile Strength, Ultimate 7.60 MPa
1100 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0460 GPa
6.67 ksi
1% Secant, ASTM D790
Tensile Impact Strength 282 kJ/m²
134 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 85.0 °C
185 °F
Exxon Method
Vicat Softening Point 55.0 °C
131 °F
1000g; ASTM D-1525