Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 48.0 °C | 118 °F | |
Advanced Elastomer Systems VistaFlex® 641N Thermoplastic Rubber
(discontinued **) A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vica.. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | Rate B; ASTM D1525 |
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | Rate B; ASTM D1525 |
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-761 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymer designed for high filler acceptance. Compounds produced from this resin have excellent flexibility and toughness.Appl.. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-767 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low gel 29.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile.. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 9320W Ionomer Resin, Zinc
(discontinued **) Surlyn® 9320W thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. This very low modulus zinc.. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | ISO 306 |
Lubrizol Advanced Materials Pearlthane® D91F88 Thermoplastic Polyurethane Elastomer Type: Pearlthane® D91F88 is an aliphatic-based thermoplastic polyurethane.Main Application : ExtrusionSpecial features : Outstanding abrasion loss, excellent color stability upon weather exposure.. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | VST/B/50; ISO 306 |
Styrolution Styrolux® 693 D SBC Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, e.. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | ASTM D1525 |
DuPont Bynel® 3860 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent .. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | B (50N); ISO 306 |
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed.. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Vicat Softening Point | 48.0 °C | 118 °F | ASTM D1525, ISO 306 |
DuPont™ Surlyn® 9320 Zinc Ionomer Surlyn® 9320 is a zinc ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 9320 thermoplastic resin .. |
|||
Vicat Softening Point | 47.8 °C | 118 °F | ASTM D1525 |
ExxonMobil OPTEMA™ TC 120 Molding Ethylene Methyl Acrylate Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer, which can be used as an impact modifier or compatibilizer in polymer compounds. TC 120 has been processed on typical LDPE.. |
|||
Vicat Softening Point | 47.8 °C | 118 °F | ASTM D1525 |
ExxonMobil Polybilt™ Bitumen Modifier 101 Low Density Polyethylene Resin Product Description: Polybilt 101 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 10.. |
|||
Vicat Softening Point | 47.8 °C | 118 °F | ASTM D1525 |
ExxonMobil Escorene™ 768.MJ Blown Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 768.MJ is a low gel 26.2% vinyl acetate copolymer designed for film and compounding applications. This resin provides very low modulus films with high tensile .. |
|||
Vicat Softening Point | 48.0 °C @Load 1.02 kg |
118 °F @Load 2.25 lb |
ASTM D1525 |
Arkema Group LOTRYL® 20 MBG 08 Copolymer Ethylene - Methyl Acrylate LOTRYL® 20MBG08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MBG 08 is a polyme.. |
|||
Vicat Softening Point | 48.0 - 90.0 °C | 118 - 194 °F | Average value: 74.4 °C Grade Count:12 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an.. |