Material Notes:
Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer, which can be used as an impact modifier or compatibilizer in polymer compounds. TC 120 has been processed on typical LDPE compounding equipment at temperatures up to 625°F.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesApplications: CompatibilizerEngineering thermoplastic Impact modifierHot Melt AdhesivesInjection MoldingMasterbatch Base ResinSoft, molded partsSound Deadening FoamInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.943 g/cc
0.0341 lb/in³
ExxonMobil Method
Methyl Acrylate Content 21.5 %
21.5 %
Melt Flow 6.00 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.00 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
15s; ASTM D2240
Hardness, Shore D 28
28
15s; ASTM D2240
Tensile Strength at Break 5.86 MPa
850 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0331 GPa
4.80 ksi
1% secant; ASTM D790
Impact Test 17.6 J

@Temperature 23.0 °C
13.0 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
28.5 J

@Temperature -40.0 °C
21.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
Thermal Properties Metric English Comments
Melting Point 77.2 °C
171 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 47.8 °C
118 °F
ASTM D1525