Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 84.0 °C @Load 1.00 kg |
183 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® MQ 10 R Low Density Polyethylene - Injection Molding Riblene MQ 10 R is a good fluidity low density polyethylene resin (LDPE).Parts made with Riblene MQ 10 R are characterized by a high flexibility.Main Applications: Riblene MQ 10 R is suitable for i.. |
|||
Vicat Softening Point | 84.0 °C @Load 1.00 kg |
183 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® MR 10 Low Density Polyethylene - Injection Molding Riblene MR 10 is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 are characterized by a high flexibility.Main Applications: Riblene MR 10 is suitable for injecti.. |
|||
Vicat Softening Point | >= 84.0 °C | >= 183 °F | ASTM D1525 |
NIZHNEKAMSKNEFTEKHIM 825 High Impact Polystyrene Grade 825 is a high impact polystyrene for injection molding. The polymer's ability to be molded on fast cycles with minimal stresses results in outstanding impact retention. It is used in such ap.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
Ineos Nova 3900 General Purpose Crystal Polystyrene
(discontinued **) High flow, Good compoundingApplications: Color concentrates, Compounding, Thin wall moldingsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and o.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-701 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt, 10.5% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughnes.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50°C/hr; 50N |
Arkema Group Oroglas® HFI-10 Acrylic, Impact Grade
(discontinued **) OROGLAS HFI-10 is an impact grade that in addition to its superior impact resistance provides an improvement in flow which contribute to improve molding behavior and reduce cycle time.Key features :.. |
|||
Vicat Softening Point | 84.0 - 118 °C | 183 - 244 °F | Average value: 99.9 °C Grade Count:29 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
LyondellBasell Petrothene® NA204000 Low Density Polyethylene ApplicationsPETROTHENE NA 204-000 is a general-purpose resin recommended for intermediate and light-weight coating applications at high speeds. NA 204-000 can be drawn down to weights of 2.0 lb/rea.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
LyondellBasell Petrothene® NA206000 Low Density Polyethylene ApplicationsPETROTHENE NA 206-000 is an extrusion coating resin especially recommended for high-speed, light weight coating applications. The resin can be drawn to a 3 lb/ream coating weight at lin.. |
|||
Vicat Softening Point | 84.0 °C @Load 5.00 kg |
183 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Vicat Softening Point | 84.0 °C @Load 5.00 kg |
183 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical AF312C ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ISO 306A |
Lucite International Elvakon® 4490 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | VST/B/50; ISO 306 |
Styrolution Polystyrol 143 E GR 2 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | VST/B/50; ISO 306 |
Styrolution Polystyrol 143 E GR 21 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 175A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ISO 306 |
Stir SpA RH I P (PVC) Application: Spiral extrusion - various profilesInformation provided by STIR SpA |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
DuPont Bynel® 41E687 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ISO 306 |
Total LDPE 1700 MN 18 C Low Density Polyethylene - Injection Molding and Compounding LDPE 1700 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade for easy flow injection molding of flexible parts, powder production for grindin.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total PSI 8350 High Impact Polystyrene 8350 is a very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is proposed for the produc.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating 7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion .. |
|||
Vicat Softening Point | 84.0 °C @Load 1.00 kg |
183 °F @Load 2.20 lb |
ASTM D1525 |
Eastman Eastar DN001HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50N; ISO 306 |
Denka TH-11 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50N; ISO 306 |
Denka TH-23 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR8020 Standard Adipate Ester Polyurethane The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion resistanceGr.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | |
BASF Polystyrol® 143 E Polystyrene (Europe) Medium strength, easy flowing general-purpose grade, suitable for blending with impact-modified Polystyrol, Styrolux and as a coextruded glossy capping layer.Data was collected by ISO methods and pr.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1020 VB 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for transparent, resistant films, sealable at low temperature. Examples: laminates.ISO data provided by the manufacturer, Arke.. |
|||
Vicat Softening Point | 84.0 - 128 °C | 183 - 262 °F | Average value: 91.9 °C Grade Count:44 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50°C/h; 50N; 10x10x4mm; ISO 306/B50 |
SYNTHOS Krasten® 552M High Impact Polystyrene High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
DuPont Bynel® 3933 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |