Vicat Softening Point 247 °C
477 °F
B
Plastcom SLOVAMID 6 GF 20 GB 10 PA6, 20% glass fibre, 10% glass beads
FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre and 10% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri..
Vicat Softening Point 247 °C
477 °F
Rate B/120; ISO 306
SABIC Innovative Plastics EXTEM XH1015 TPI Resin
Thermoplastic Polyimide Extem* XH1015 Resin.
Vicat Softening Point 247 °C
477 °F
Rate B/120; ISO 306
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Asia Pacific)
Thermoplastic Polyimide Extem* XH1015 Resin.
Vicat Softening Point 247 °C
477 °F
Rate B/120; ISO 306
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1015 Resin.
Vicat Softening Point 247 °C
477 °F
Rate B/120; ISO 306
SABIC Innovative Plastics EXTEM XH1015F TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1015 Resin. EFSA food Contact approved.
Vicat Softening Point 247 °C
477 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET
LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications.
Vicat Softening Point 247 °C
477 °F
B/120; ISO 306
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Vicat Softening Point 247 °C
477 °F
B/50; ISO 306
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding
Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Vicat Softening Point 247 °C
477 °F
50°C/h 50N; ISO 306
LATI LATILUB 80-40GRT Polyphenylene sulfide Base (PPS), 40% Graphite and PTFE Self Lubricating Plastic  (U