Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 45.0 MPa @Temperature 275 °C |
6530 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
Flexural Strength | 45.0 MPa @Temperature 80.0 °C |
6530 psi @Temperature 176 °F |
Practical Use (Water Absorption 3.0%); ASTM-D790 |
Toyobo GLAMIDE® T-400G15 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 45.0 MPa @Temperature 23.0 °C |
6530 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 3.0%); ASTM-D790 |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 45.0 MPa @Temperature 80.0 °C |
6530 psi @Temperature 176 °F |
Practical Use (Water Absorption 1.9%); ASTM-D790 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 45.0 MPa @Temperature -40.0 °C |
6530 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.0%); ASTM-D790 |
Toyobo GLAMIDE® T-222SA Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 45.0 MPa @Temperature 150 °C |
6530 psi @Temperature 302 °F |
ISO 178 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Flexural Strength | 45.0 MPa @Temperature 275 °C |
6530 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |
|||
Flexural Strength | 45.0 MPa @Temperature 275 °C |
6530 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |