Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 180 MPa @Temperature -40.0 °C |
26100 psi @Temperature -40.0 °F |
ISO 178 |
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**) Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr.. |
|||
Flexural Strength | 180 MPa @Temperature 175 °C |
26100 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Flexural Strength | 180 MPa @Temperature 23.0 °C |
26100 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Flexural Strength | 180 MPa @Temperature 125 °C |
26100 psi @Temperature 257 °F |
ISO 178 |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
Flexural Strength | 180 MPa @Strain 5.00 % |
26100 psi @Strain 5.00 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 180 MPa @Temperature 23.0 °C |
26100 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.0%); ASTM-D790 |
Toyobo GLAMIDE® T-403 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 180 MPa @Temperature 23.0 °C |
26100 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 180 MPa @Temperature 80.0 °C |
26100 psi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 180 MPa @Temperature 23.0 °C |
26100 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |