Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 8.76 kN/m | 50.0 pli | ASTM D624 |
PolyOne Versaflex™ CL2000X Thermoplastic Elastomer (TPE) Versaflex™ CL2000X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and an extremely soft feel are desired. - Tactile Feel - Ultra-Soft - Water Clar.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit NC-Consil® 750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit SC-Consil® FR861 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit SC-Consil® FR862 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Die B |
Malvern Minerals Sliastic 740 with 33% Novacite® Daper Quartz Filler Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Die B |
Malvern Minerals Sliastic 740 with 33% Novacite® L-207A Quartz Filler Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 25-9000 TPE Product Description: StarGrip GP 25-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubber.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® 2345-2 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M783 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M832 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M98 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 3 Tear Resistant PTFE-Coated Glass Description: Chemfab® Tear Resistant Series is manufactured with specialized coating materials to improve tear and crease resistance. Uses for this series includes release sheets, belting and gas.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® K350 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® SlipGrip™ 3 PTFE/Silicone Coated Fiberglass Fabric Description: SlipGrip™ products are PTFE-coated fiberglass fabrics with silicone rubber on one face. This unique combination provides a "slippery" PTFE surface and a "grippy" silicone surface. .. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Teknor Apex UNIPRENE® 2021 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | |
Dow Corning SILASTIC® L RTV SILICONE RUBBER BASE & CURING AGENT Low durometer silicone mold making rubber recommended for use with rigid polyurethanes and can be used with polyesters and epoxies.Information provided by Dow Corning |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit SC-Consil® 861 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3820M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentApplications:FDA (Food Contact)Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingDisclaimer: A thermoplasti.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Die B; silicone property; ASTM D624 |
Arlon R37879X034 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass |