Material Notes:
Description/Features:High Performance Thermoplastic ElastomerTransparentApplications:FDA (Food Contact)Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingDisclaimer: A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in accordance with accepted test methods. All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21 for use in the packaging of food. The listings cover many uses and restrictions may apply depending on the application. PLEASE CONTACT US TO REVIEW THE SUITABILITY OF SPECIFIC PRODUCTS IN SPECIFIC APPLICATIONS. This statement is only an overview of the FDA listings for this product. IT IS THE CUSTOMER'S RESPONSIBILITY TO ENSURE THAT THE COMPOUND IS SUITABLE FOR ITS INTENDED APPLICATIONS.Information provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 20
20
Instant; ASTM D2240
Tensile Strength, Yield 3.17 MPa
460 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
0.621 MPa

@Strain 300 %
90.0 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 760 %
760 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Rebound 63 %
63 %
Bayshore; ASTM D2632
Tear Strength 8.77 kN/m
50.0 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 27 %
27 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -65.0 °C
-85.0 °F
ASTM D746