Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 31.5 kN/m | 180 pli | ASTM D624 |
Multibase Multi-Flex® TPE G 7155 BLK Multi-Flex® G 7155 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactu.. |
|||
Tear Strength | 31.5 kN/m | 180 pli | ASTM D624 |
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp.. |
|||
Tear Strength | 31.5 kN/m | 180 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90250 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 31.5 kN/m | 180 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible 90461 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 31.5 kN/m | 180 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible D7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 31.6 kN/m | 180 pli | 73°F; ASTM D624 |
Advanced Elastomer Systems VistaFlex® 714-N Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Tear Strength | 31.5 kN/m | 180 pli | ASTM D624 |
PolyOne Dynaflex™ G2703-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2703-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance and a low coefficient of friction. - Adhesion to Polypropylen.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-265 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 31.6 kN/m | 180 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-515 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 31.6 kN/m | 180 pli | Die C |
Taiwan PU Corporation UR50 Polyester Urethane Rubber UR50 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Tear Strength | 31.6 kN/m | 180 pli | Die B |
Shin-Etsu Silicones KE-5006BU Low Temperature Silicone Elastomer ShinEtsu KE5006B U is a phenyl (PVMQ) silicone compound. This product is designed for good low temperature characteristics.Product Features: A broad range of service temperatures from 100 to +260°.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 55-HR-9 TPE Product Description: StarTUFF TF 55-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | JIS K6301-B |
Stellarchem AB870LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | Initial Tear Strength |
Saint-Gobain CHR® H7575 Glass-Silicone Backing Silicone Adhesive Pressure Sensitive Tape Description: Silicone glass provides temperature resistance from -85°F to +500°F (-62°C to +260°C) and exceptional tensile strength and abrasion resistance. Applications include thermal .. |
|||
Tear Strength | 31.6 kN/m | 180 pli | Fill/Transverse direction |
Saint-Gobain COHRlastic® 1015 General-Purpose Electrical-Grade Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-1522G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tear Strength | 31.6 kN/m | 180 pli | Trouser; ASTM D470 |
Lubrizol Estane® 58246 Thermoplastic Polyurethane Features: High stiffness grade with excellent chemical and oil resistance.Uses: Flat Die/Cast Film Extrusion and Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaI.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | Die C; ASTM D 624 |
CPT C-Flex® R70-072 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | |
Dow Corning SILASTIC® T-4 RTV SILICONE RUBBER BASE & T-4 O CURING AGENT Translucent, oil bleeding high strength silicone mold making rubber that features high tear with fast cure. Suited for prototype design and production tooling. Silastic T-4 O is recommended for use .. |
|||
Tear Strength | 31.6 kN/m | 180 pli | |
Dow Corning SILASTIC® V RTV SILICONE RUBBER BASE & CURING AGENT High strength silicone rubber featuring medium durometer, low mixed viscosity, suited for the reproduction of architectural, furniture components and prototypes. Silastic V is recommended for use wi.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 Dense Extruded Profile FormulationNordel® IP 5565 |
|||
Tear Strength | 31.6 kN/m | 180 pli | ISO 34-1 |
Alliance Polymers Viprene™ P50A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P50A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | ISO 34-1 |
Alliance Polymers Viprene™ P50A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P50A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | ASTM D624 |
Buckeye Polymers BP Flex D0840 TPO Replace Flex PVCTPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resis.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | ISO 34-1 |
Alliance Polymers Viprene™ G55A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G55A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 31.6 kN/m | 180 pli | Die C; ASTM D624 |
Aaron Industries AAROPRENE® ATPR 1000 60A Elastomeric Compound AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified. |
|||
Tear Strength | 31.6 kN/m | 180 pli | ASTM D624 |
Multibase Multi-Flex® A 6202 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |