Mechanical Properties Metric English Comments
Tear Strength 29.8 kN/m
170 pli
ASTM D624
Multibase Multi-Flex® TPE A 7321 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 29.8 kN/m
170 pli
ASTM D412
Multibase TPSiV™ 3010-60A Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
Tear Strength 29.8 kN/m
170 pli
ASTM D624
PolyOne Dynaflex™ G7670-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7670-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Tear Strength 29.8 kN/m
170 pli
ASTM D624
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tear Strength 29.8 kN/m
170 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible A6500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Tear Strength 29.8 kN/m
170 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible B65T0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tear Strength 29.8 - 114 kN/m
170 - 650 pli
Average value: 67.6 kN/m Grade Count:16
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..
Tear Strength 29.8 kN/m
170 pli
Die C, 510 mm/min; ASTM D624
PolyOne Elastamax™ HTE 1104 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco..
Tear Strength 29.8 kN/m
170 pli
Injection molded plaques, Die C, Cross Direction; ASTM D624
Kraton® G2705 GU (SEBS) Compound
Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good punct..
Tear Strength 29.8 kN/m
170 pli
ASTM D624
Multibase Multi-Flex® G 7430 TPE Styrene Ethylene Butylene Styrene Block Copolymer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Tear Strength 29.8 kN/m
170 pli
Die B, post cured- 8 hours at 177°C; ASTM D624
Multibase C6-235 VAROX DBPH Dow-Corning Class VI Elastomer
Information provided by Multibase
Tear Strength 29.8 kN/m
170 pli
Die B,post cured- 2 hours at 177°C; ASTM D624
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer
Information provided by Multibase
Tear Strength 29.8 kN/m
170 pli
ASTM D624
Multibase Multi-Flex® A 5003 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Tear Strength 29.8 kN/m
170 pli
ASTM D624
Multibase Multi-Flex® A 7101 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Tear Strength 29.8 kN/m
170 pli
ASTM D624
Multibase Multi-Flex® A 7206 E TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Tear Strength 29.8 kN/m
170 pli
ASTM D624
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1060 TPE
Product Description: StarCLEAR CLR-1060 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat..
Tear Strength 29.8 kN/m
170 pli
ASTM D624
Teknor Apex Telcar® TL-6800-73 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tear Strength 29.8 kN/m
170 pli
Trouser; ASTM D470
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Tear Strength 29.8 kN/m
170 pli16 %
16 % 200% elongation; ASTM D412
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane
Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection ..
Tear Strength 29.8 kN/m
170 pli
Trouser; ASTM D470
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane
Features: Very good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion Available in Americas, Europe,..
Tear Strength 29.8 kN/m
170 pli
Dow Corning HV 1520/40
40 Shore Hardness Conductive liquid silicone rubber with high tear strength, high electrical conductivity and fast cure speedInformation provided by Dow Corning
Tear Strength 29.8 kN/m
170 pli
Dow Corning HV 1540/20P BASE AND CLEAR CURING AGENT
32 Shore, very low viscosity, castable hydrophobic silicone rubber with high tear strength and low temperature cure.Information provided by Dow Corning
Tear Strength 29.8 kN/m
170 pli
ASTM D624
Diamond Polymers Softflex® 2701-1502R
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tear Strength 29.8 kN/m
170 pli
ASTM D624
Diamond Polymers Softflex® SF 5060 Overmold for Nylon
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tear Strength 29.8 kN/m
170 pli
ASTM D470
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane
Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b..
Tear Strength 29.8 kN/m
170 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® IT 38-082 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerOver-Molding GradeTransparentMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided b..
Tear Strength 29.8 kN/m
170 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-5165 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalIgnition ResistantApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Injection Mo..
Tear Strength 29.8 kN/m
170 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® ST-6240 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Over-Molding GradeUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.