Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 6821 C BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | >= 24.5 kN/m | >= 140 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 7606 BLK The burn rate is 1.2 in/min (30 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 24.5 kN/m | 140 pli | post cured- 2 hours at 177°C; Die B |
Multibase SILASTIC® C7-4535 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Tear Strength | 24.5 - 26.5 kN/m | 140 - 151 pli | ASTM D624 |
Proto3000 Objet Digital Materials™ DM_9885/9785 Rubber-like Prototyping Polymer Primary material: TangoBlackPlus/TangoPlusSecondary material: VeroWhitePlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structu.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
PolyOne Dynaflex™ D3202-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3202-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel -.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
PolyOne Dynaflex™ G7960-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-235 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7370-1000 TPE Product Description: StarFlex P 7370-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | |
Dow Corning SILASTIC® 7-6830 BIOMEDICAL GRADE LSR, KIT Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning |
|||
Tear Strength | 24.5 kN/m | 140 pli | |
Dow Corning SILASTIC® Q7-4535 BIOMEDICAL GRADE ETR ELASTOMER One-part, enhanced tear-resistant silicone elastomers; uncatalyzed (customer selects peroxide catalyst) elastomer materials designed for compounding into elastomer for part fabrication and medical d.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | at 25°C |
Daikin DAI-EL G-501NK Fluoroelastomer Terpolymer, Diamine Curable Grade, 68% Fluorine Content Features: Good mechanical characteristics.Information provided by Daikin Industries. |
|||
Tear Strength | 24.5 kN/m | 140 pli | at 25°C |
Daikin DAI-EL G-716 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Minimal compression set and fast vulcanization.Information provided by.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | kg/cm²; JIS-K-6301 |
Denka LCS Z6050 Thermoplastic Elastomer, Injection Molding Grade (general) "DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4570 General Purpose Compound FormulationNordel® IP 4570 |
|||
Tear Strength | 24.5 kN/m | 140 pli | Fill, Breaking Strength w/o Sizing |
3M Nextel™ AF-10 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tear Strength | 24.5 kN/m | 140 pli | B, cured 72 hrs @ RT |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Warp, Breaking Strength w/o Sizing |
3M Nextel™ AF-11 Aerospace Woven Fabric 312 Information provided by 3M |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 702 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection MoldingPolyOne.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3860E Thermoplastic Elastomer - SBC
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | die B; ASTM D624 |
G-2705 Styrene-based Biomedical Elastomer |