Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 15.8 kN/m | 90.2 pli | ASTM D624 |
PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3226-1000-03 is an easy processing TPE designed for general purpose applications. It is suitable for injection molding, extrusion, blow molding and thermoforming processes. - Dry Feel - .. |
|||
Tear Strength | 15.8 kN/m | 90.2 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible C6501 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; silicone property; ASTM D624 |
Arlon A3020-T004-12 Silicone Rubber/Fiberglass Laminate
(discontinued **) Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon A1030-R008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape
(disco 2 inches width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon A3015-R004-12 0.015" (0.381 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
  1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film This.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-230A Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 3 High-Performance PTFE-Coated Glass Description: Chemfab® High-Performance Series provides the highest level of PTFE content for superior surface smoothness, durability, and longer life. Use this product for the most demanding heat.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 500F PTFE Coated Beta Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi.. |
|||
Tear Strength | 15.8 kN/m | 90.2 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-6055 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tear Strength | 15.8 kN/m | 90.2 pli | ASTM D624 |
Teknor Apex Uniprene® UN-7100-55 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | |
Cytec EN-12 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon 48101R008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cured Silicone RubberInterleave 2: Polyethylene Product Use: Flexible heater insul.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | [ppiw], Silicone Property; ASTM D624 |
Arlon 55142R040 0.040" (1.02 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be use.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | [ppiw], Silicone Property; ASTM D624 |
Arlon 56146R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon R37642R062 0.062" (1.57 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Interleave: PolyethyleneSide 1: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, mater.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | ASTM D624 |
Arlon R39091R036 0.036" (0.914 mm) Uncured Silicone Rubber with Nomex Fabric Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1574 Nomex FabricSide 2: Uncured SiliconeInterleave: Polyethylene This data represents typical values fo.. |
|||
Tear Strength | 15.8 kN/m @Temperature 25.0 °C, Time 259000 sec |
90.0 pli @Temperature 77.0 °F, Time 72.0 hour |
B, Cured |
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | silicone property; ASTM D624 |
Arlon 51141R020 Silicone Rubber/Fiberglass Laminate Interleave 1: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon 51273R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: Polyethylene This data represents typical values for the production materia.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; silicone property; ASTM D624 |
Arlon 51276R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, layer 2; ASTM D624 |
Arlon 55109R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Layer 1, Die B, [ppiw], Silicone Property; ASTM D624 |
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | [ppiw], Layer 1, Die B, Silicone Property; ASTM D624 |
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; silicone property; ASTM D624 |
Arlon 55279R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon 31140R020 0.020" (0.508 mm) Uncured Fluorosilicone Rubber on Release Carrier Design/Construction: Interleave: PolyethyleneProduct: Uncured Fluorosilicone Rubber Carrier: Release coated HDPE Product Use: Flexible heater insulationAppearance: Red silicone gum on polymer releas.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; Silicone Property; Arlon SQA-TMS-029 |
Arlon 32140R060 0.060" Uncured Silicone Rubber on Release PET Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be use.. |