Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0004905 - 0.0014715 GPa @Temperature 500 °C, Time 10800 sec |
0.07114 - 0.21343 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-100S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0004905 - 0.0014715 GPa @Temperature 500 °C, Time 10800 sec |
0.07114 - 0.21343 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-110S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0004905 - 0.0014715 GPa @Temperature 1000 °C, Time 10800 sec |
0.07114 - 0.21343 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories INCT-120N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0004905 - 0.0024525 GPa @Temperature 500 °C, Time 10800 sec |
0.07114 - 0.35571 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-120S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0004905 - 0.0024525 GPa @Temperature 1000 °C, Time 10800 sec |
0.07114 - 0.35571 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories INCT-135N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0004905 - 0.0024525 GPa @Temperature 500 °C, Time 10800 sec |
0.07114 - 0.35571 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT135S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0004905 - 0.000981 GPa @Temperature 500 °C, Time 10800 sec |
0.07114 - 0.142 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-50S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0004905 - 0.000981 GPa @Temperature 500 °C, Time 10800 sec |
0.07114 - 0.142 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-80N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0004905 - 0.000981 GPa @Temperature 1000 °C, Time 10800 sec |
0.07114 - 0.142 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories MIX-2 Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |