Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.017658 GPa @Temperature 1500 °C, Time 10800 sec |
2.5611 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories CTC-63TD Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.017658 GPa @Temperature 110 °C, Time 86400 sec |
2.5611 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.017658 GPa @Temperature 110 °C, Time 86400 sec |
2.5611 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HSC-16H-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.017658 GPa @Temperature 1000 °C, Time 10800 sec |
2.5611 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HSC-16S-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.017658 GPa @Temperature 1000 °C, Time 10800 sec |
2.5611 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SFC-60 SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.017658 GPa @Temperature 110 °C, Time 86400 sec |
2.5611 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SFC-90W High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.017658 GPa @Temperature 1500 °C, Time 10800 sec |
2.5611 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories PCT-AM-1 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |