Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0118 GPa @Temperature 1500 °C |
1.71 ksi @Temperature 2730 °F |
|
Sharadaa Ceramics REFCAST HA High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Modulus of Rupture | 0.0118 GPa @Temperature 110 °C |
1.71 ksi @Temperature 230 °F |
|
Sharadaa Ceramics REFCAST LC60 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Modulus of Rupture | 0.0118 GPa @Temperature 110 °C |
1.71 ksi @Temperature 230 °F |
|
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Modulus of Rupture | 0.0118 GPa @Temperature 110 °C |
1.71 ksi @Temperature 230 °F |
|
Sharadaa Ceramics REFCAST ULCC90 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Modulus of Rupture | 0.0118 GPa @Temperature 110 °C |
1.71 ksi @Temperature 230 °F |
|
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Modulus of Rupture | 0.0118 GPa @Temperature 110 °C |
1.71 ksi @Temperature 230 °F |
|
Sharadaa Ceramics THERMO PATCH EXCEL High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |