Mechanical Properties Metric English Comments
Flexural Modulus 20.0 - 22.0 GPa
2900 - 3190 ksi
ISO 178
Raschig Group EN 5004 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Flexural Modulus 20.0 - 22.0 GPa
2900 - 3190 ksi
ISO 178
Raschig Group EN 5007 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Flexural Modulus 18.0 - 22.0 GPa
2610 - 3190 ksi
Injection; ISO 178
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Flexural Modulus 9.00 - 22.0 GPa
1310 - 3190 ksi
Average value: 14.0 GPa Grade Count:6
Overview of materials for Phenolic/Glass Fiber SMC
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Glass Fiber SMC". Each property range of values reported is minimum and maximum values of appro..
Flexural Modulus 9.30 - 22.0 GPa
1350 - 3190 ksi
Average value: 14.4 GPa Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Flexural Modulus 17.0 - 22.0 GPa
2470 - 3190 ksi
Longitudinal
Goodfellow Polyaramid/Vinylester Composite Tube or Rod
Information provided by Goodfellow.
Flexural Modulus 18.0 - 22.0 GPa
2610 - 3190 ksi
Injection; ISO 178
Raschig Group RESINOL® 400 EPF Phenolic