Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.83 - 19.3 GPa | 700 - 2800 ksi | Average value: 9.22 GPa Grade Count:21 |
Overview of materials for Polycarbonate, NCG Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Flexural Modulus | 1.55 - 19.3 GPa | 225 - 2800 ksi | Average value: 2.35 GPa Grade Count:214 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Flexural Modulus | 0.103 - 19.3 GPa | 14.9 - 2800 ksi | Average value: 5.43 GPa Grade Count:176 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Flexural Modulus | 8.27 - 19.3 GPa | 1200 - 2800 ksi | Average value: 14.8 GPa Grade Count:20 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Flexural Modulus | 2.90 - 19.3 GPa | 420 - 2800 ksi | Average value: 8.67 GPa Grade Count:46 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Flexural Modulus | 17.2 - 19.3 GPa | 2500 - 2800 ksi | Average value: 18.1 GPa Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% .. |
|||
Flexural Modulus | 2.76 - 19.3 GPa | 400 - 2800 ksi | Average value: 8.51 GPa Grade Count:18 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |