| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 0.103 GPa | 14.9 ksi | ASTM D790 |
|
PolyOne Edgetek® PF-05GF/000 FR MR Polysulfone (PSU)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Flexural Modulus | 0.103 GPa | 14.9 ksi | Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790 |
|
Phillips Sumika Marlex® CHP-015 Thermoplastic Polyolefin
(discontinued **)
Applications: Driver-side air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 201..
|
|||
| Flexural Modulus | 0.103 GPa | 14.9 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
|
Eastman 812A Polyethylene
(discontinued **)
Polyethylene 812A is a natural low density material with a 200 melt index. This high-flow formulation is used for specialty injection molding applications in the medical market.Unless otherwise not..
|
|||
| Flexural Modulus | 0.103 GPa | 14.9 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
|
Eastman 812P Polyethylene
(discontinued **)
Polyethylene 812A is a natural low density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a carpet backing to bind fibers to the carpet...
|
|||
| Flexural Modulus | 0.103 - 19.3 GPa | 14.9 - 2800 ksi | Average value: 5.43 GPa Grade Count:176 |
|
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
|
|||