Flexural Modulus 16.0 - 18.0 GPa
2320 - 2610 ksi
Injection; ISO 178
Raschig Group 2557 AMC Polyester
Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low ..
Flexural Modulus 16.0 - 18.0 GPa
2320 - 2610 ksi
Injection; ISO 178
Raschig Group 2568 AMC
Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s..
Flexural Modulus 16.0 - 18.0 GPa
2320 - 2610 ksi
Injection; ISO 178
Raschig Group 2572 AMC
Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin..
Flexural Modulus 14.0 - 18.0 GPa
2030 - 2610 ksi
Injection and Compression; ISO 178
Raschig Group 3536 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Flexural Modulus 12.0 - 18.0 GPa
1740 - 2610 ksi
Injection; ISO 178
Raschig Group 5553 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Flexural Modulus 14.0 - 18.0 GPa
2030 - 2610 ksi
Injection; ISO 178
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Flexural Modulus 14.0 - 18.0 GPa
2030 - 2610 ksi
Injection; ISO 178
Raschig Group DECAL® 666/8/2B Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe..
Flexural Modulus 8.00 - 18.0 GPa
1160 - 2610 ksi
Average value: 13.1 GPa Grade Count:26
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..
Flexural Modulus 16.0 - 18.0 GPa
2320 - 2610 ksi
Compression; ISO 178
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Flexural Modulus 7.00 - 18.0 GPa
1020 - 2610 ksi
Average value: 14.3 GPa Grade Count:8
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..
Flexural Modulus 16.0 - 18.0 GPa
2320 - 2610 ksi
Compression; ISO 178
Raschig Group RESINOL® 400 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Flexural Modulus 16.0 - 18.0 GPa
2320 - 2610 ksi
Injection; ISO 178
Raschig Group 5557 DAP  (discontinued **)
Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h..
Flexural Modulus 4.30 - 18.0 GPa
624 - 2610 ksi
Average value: 8.46 GPa Grade Count:15