Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.600 GPa | 87.0 ksi | ASTM D790 |
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ASTM D790 |
Reliance Industries Relene S42005 Polyethylene Wire and cable High Density Polyethylene grade. Characteristics: excellent processing, superior physical/electrical properties, good environmental stress crack resistance. Applications: recommended .. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ASTM D790 |
Reliance Industries Relene W43006 Polyethylene Relene W43006 is a polyethylene grade recommended for insulation in jelly filled telecommunication cables. This grade contains a special stabilization system for improved thermal resistance. It is.. |
|||
Flexural Modulus | 0.600 - 0.600 GPa @Temperature 90.0 - 90.0 °C |
87.0 - 87.0 ksi @Temperature 194 - 194 °F |
Average value: 0.600 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2508-UV9 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.600 - 4.30 GPa @Temperature -40.0 - 90.0 °C |
87.0 - 624 ksi @Temperature -40.0 - 194 °F |
Average value: 1.92 GPa Grade Count:4 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 115-1332 LMDPE Rotational Molding Resin Description: ICORENE 115-1332 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | 1.33 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 190-1332 LMDPE Rotational Molding Resin Description: ICORENE 190-1332 is a compounded linear density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness.. |
|||
Flexural Modulus | 0.600 GPa @Temperature 23.0 °C |
87.0 ksi @Temperature 73.4 °F |
ISO 178 |
MBA Polymers HDPE 1107 E Post-consumer recycled fractional melt high density polyethylene Available in standard black.Information provided by MBA Polymers. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ISO 178 |
Solvay TECHNYL® C 52G4 MZ25 PA6, 25% mineral filler, DRY Description: TECHNYL® C 52G4 MZ25 is a 25% mineral reinforced melamine cyanurate flame retarded polyamide 6.This product is heat stabilized and is suitable for injection molding. This product is .. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP) LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s). |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | 50% humidity; ISO 178 |
Borealis Borseal™ RE239CF Polypropylene Copolymer Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high.. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ASTM D 790 |
Total Lumicene® M 3410 EP HDPE Film, sheet FINACENE® M 3410 EP is a medium density metallocene based polyethylene resin. FINACENE® M 3410 EP is especially dedicated to film applications where a higher rigidity, good transparency and shrink.. |
|||
Flexural Modulus | 0.600 GPa @Temperature 80.0 °C |
87.0 ksi @Temperature 176 °F |
ASTM D790 |
Toyobo T-661 Nylon 66, Standard Grade (Conditioned) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ASTM D790 |
UBE UBESTA® 3030JLX2 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: semi-plasticized, UV resistance, heat resistanceInformation provided by UBE. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ASTM D 790 |
Total Lumicene® mPE M 3410 EP HDPE Film Outstanding clarity and gloss; excellent bubble stability; excellent tear strength; high puncture resistance; good stiffness; excellent heat sealing properties; excellent compatibility with LDPE and.. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ISO 178 |
Chengdu Polyster H8570 Thermoplastic Polyether-ester Elastomer (TPEE) High modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent heat-ageing resistance and toughness. Applications requiring high strength, high toughness and good .. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ASTM D790 |
Covestro Bayflex® 110-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Flexural Modulus | 0.600 GPa @Temperature 160 °C |
87.0 ksi @Temperature 320 °F |
ISO 178 |
DSM Stanyl® TS300 PA46 |
|||
Flexural Modulus | 0.600 GPa @Temperature 160 °C |
87.0 ksi @Temperature 320 °F |
ISO 178 |
DSM Stanyl® TW341-B PA46 Heat Stabilized, Lubricated |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | 1% secant; ASTM D790 |
ExxonMobil LL 8360.29 Rotational Molding Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Flexural Modulus | 0.600 GPa @Temperature 65.0 °C |
87.0 ksi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8202C PA6 (Dry) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ASTM D790 |
Chem Polymer Chemlon 256 Nylon 6, Wire Jacketing Grade A non-halogenated, Allwires rated wire coating grade used primarily on cables for power and control circuits in commercial and industrial applications. The cables are oil, gasoline, and abrasion re.. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ASTM D790 |
3M Dyneon™ PFA FLEX 8502 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules Dyneon™ PFA-FLEX UHP family exhibits improved environmental stress crack resistance to stress cracking agents such as fluorsurfactants and fluorosurfactant-containing chemicals. In addition, this f.. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ASTM D790 |
Asahi Glass Fluon® P-830UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Flexural Modulus | 0.600 - 0.600 GPa @Temperature 90.0 - 90.0 °C |
87.0 - 87.0 ksi @Temperature 194 - 194 °F |
Average value: 0.600 GPa Grade Count:1 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | SAE J949 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (6 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.600 - 1.15 GPa | 87.0 - 167 ksi | Average value: 0.875 GPa Grade Count:30 |
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Rotational Molding Grade". Each property range of values reported is m.. |
|||
Flexural Modulus | 0.600 GPa | 87.0 ksi | ISO 178 |
Unitika EX-1030 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 0.600 - 6.83 GPa @Temperature 100 - 175 °C |
87.0 - 991 ksi @Temperature 212 - 347 °F |
Average value: 2.98 GPa Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |