Mechanical Properties Metric English Comments
Flexural Modulus 0.0600 GPa
8.70 ksi
Secant 1%; ASTM D-790-95
Multibase Multi-Flex® TPO 4107 BLK
Data provided by Multibase.
Flexural Modulus 0.0600 GPa
8.70 ksi
ISO 178
Polimeri Europa Clearflex® MP D0 Very Low Density Polyethylene
Clearflex MP D0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati..
Flexural Modulus 0.0600 GPa
8.70 ksi
ISO 178
Polimeri Europa Greenflex® ML 40 Ethylene Vinyl Acetate Copolymer - Injection Molding
Greenflex ML 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding of flexible items. Items produced with Greenflex ML 40 show high elasticity and flexibility.Main Applications: Gr..
Flexural Modulus 0.0600 GPa
8.70 ksi
ASTM D790
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, e..
Flexural Modulus 0.0600 GPa
8.70 ksi
ISO 178
Huntsman AVALON® 650 B Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
Flexural Modulus 0.0600 GPa
8.70 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD855 PPE-TPE (Asia Pacific)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as cable jacket of UL 62 SPE and NISPE confiations. Flame retardant performance capable of m..
Flexural Modulus 0.0600 GPa
8.70 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP781 PPE-TPE
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..
Flexural Modulus 0.0600 GPa
8.70 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific)
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..
Flexural Modulus 0.0600 GPa
8.70 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East)
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..
Flexural Modulus 0.0600 GPa
8.70 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON TX06488NTX1 PU
LNP* STAT-KON* TX06488NTX1 is a compound based on Polyurethane resin containing Proprietary Filler(s). Added features of this grade are: Execllent Ductility, Electrically Conductive.
Flexural Modulus 0.0600 GPa
8.70 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Flexural Modulus 0.0600 GPa
8.70 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Flexural Modulus 0.0600 GPa
8.70 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Flexural Modulus 0.0600 GPa
8.70 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Flexural Modulus 0.0600 GPa
8.70 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Flexural Modulus 0.0600 GPa
8.70 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Flexural Modulus 0.0600 GPa
8.70 ksi
ISO 178
Chengdu Polyster CH4132 Thermoplastic Polyether-ester Elastomer (TPEE)
Poly-basic block copolymer. Good compatibility with POM. For blending with POM to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd.
Flexural Modulus 0.0600 GPa
8.70 ksi
ISO 178
Chengdu Polyster H4040 Thermoplastic Polyether-ester Elastomer (TPEE)
Low modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent flex resistance, especially at low temperatures. Moldable even in thin sections. Can be used in light..
Flexural Modulus 0.0600 GPa
8.70 ksi
1% secant; ASTM D790
ExxonMobil Escorene® LD 713.93 Molding, extrusion and compounding resin
Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer with very good toughness, high clarity and excellent processability. It is suitable for use in making molded articles, extruded profile..
Flexural Modulus 0.0600 GPa
8.70 ksi
ASTM D638
Arkema Group LOTADER® 3410 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3410 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3410 is a versatile adhesive for extrusion coating or lam..
Flexural Modulus 0.0600 GPa
8.70 ksi
ASTM D638
Arkema Group LOTRYL® 16 MA 003 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 16 MA 003 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 16 MA 003 is a polymer o..