Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connectors. UL 94-V0 performance with good processability. 80 Shore A hardness.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Water Absorption 0.23 %
<br>@Time 173000 sec
0.23 %
<br>@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0049 cm/cm
<br>@Time 86400 sec
0.0049 in/in
<br>@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0073 cm/cm
<br>@Time 86400 sec
0.0073 in/in
<br>@Time 24.0 hour
ASTM D955
Melt Flow 13.5 g/10 min
<br>@Load 5.00 kg,<br> Temperature 210 °C
13.5 g/10 min
<br>@Load 11.0 lb,<br> Temperature 410 °F
ASTM D1238
17.4 g/10 min
<br>@Load 2.16 kg,<br> Temperature 250 °C
17.4 g/10 min
<br>@Load 4.76 lb,<br> Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
30S reading; ASTM D2240
Tensile Strength at Break 13.0 MPa
1890 psi
Type I, 50 mm/min; ASTM D638
13.0 MPa
1890 psi
50 mm/min; ISO 527
Elongation at Break 168 %
168 %
50 mm/min; ISO 527
175 %
175 %
Type I, 50 mm/min; ASTM D638
Flexural Modulus 0.0600 GPa
8.70 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.0800 GPa
11.6 ksi
12.5 mm/min; ISO 178
Tear Strength 8.00 kN/m
45.6 pli
ISO 6383
Thermal Properties Metric English Comments
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Flammability, UL94 V-0
<br>@Thickness 6.00 mm
V-0
<br>@Thickness 0.236 in
UL 94
Oxygen Index 25 %
25 %
ISO 4589
Glow Wire Test 725 °C
1340 °F
IEC 60695-2-13
850 °C
<br>@Thickness 3.00 mm
1560 °F
<br>@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 3.80e+14 ohm-cm
3.80e+14 ohm-cm
IEC 60093
Dielectric Constant 3.1
<br>@Frequency 1.00e+6 Hz
3.1
<br>@Frequency 1.00e+6 Hz
IEC 60250
3.4
<br>@Frequency 50.0 - 60.0 Hz
3.4
<br>@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm
<br>@Thickness 2.00 mm
559 kV/in
<br>@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0020
<br>@Frequency 1.00e+6 Hz
0.0020
<br>@Frequency 1.00e+6 Hz
IEC 60250
0.0050
<br>@Frequency 50.0 - 60.0 Hz
0.0050
<br>@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 142
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 84
ASTM E 662