Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0500 GPa | 7.25 ksi | ISO 178 |
Huntsman AVALON® 92 AB Thermoplastic Polyurethane Introduction: AVALON 92 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 92 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD771 PPE-TPE (Asia Pacific) Flexible, high tensile elongation, halogen-free extrusion grade intended for evaluation in applications such as cable jacket. Flame retardant performance capable of meeting UL VW-1 requirement. 80C .. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE (Asia Pacific) Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Europe-Africa-Middle East) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | ISO 178 |
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients.. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | ISO 178 |
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | ASTM D638 |
Arkema Group LOTRYL® 18 MA 02 Copolymer Ethylene - Methyl Acrylate LOTRYL® 18 MA 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 18 MA 02 is a polymer of .. |
|||
Flexural Modulus | 0.0500 GPa | 7.25 ksi | ASTM D638 |
Arkema Group LOTRYL® 15 MA 03 Copolymer Ethylene - Methyl Acrylate LOTRYL® 15 MA 03 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 15 MA 03 is a polymer of .. |
|||
Flexural Modulus | 0.0500 GPa @Thickness 2.00 mm |
7.25 ksi @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D790 |
BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |