Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.02 GPa | 583 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-3102G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 4.02 GPa | 583 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 4.02 GPa | 583 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 4.02 GPa | 583 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-3102G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 4.02 GPa | 583 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 4.02 GPa | 583 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE) LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 4.02 GPa | 583 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 4.02 GPa | 583 ksi | ISO 178-93 |
Wellman Wellamid® WE1408 13% Glass Fiber Reinforced Engineering Grade Nylon 66 Description: Glass Fiber Reinforced Engineering Grade Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 4.02 GPa @Temperature 65.0 °C |
583 ksi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |