Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.30 GPa @Temperature 23.0 °C |
479 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A12^FC Nylon 66 Information provided by Polykemi AB |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability.. |
|||
Flexural Modulus | 3.30 - 3.30 GPa @Temperature 60.0 - 60.0 °C |
479 - 479 ksi @Temperature 140 - 140 °F |
Average value: 3.30 GPa Grade Count:2 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ISO 178 |
Nilit FRIANYL B63 W-KV30 Nylon 6 for injection molding, 30% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.30 - 7.60 GPa | 479 - 1100 ksi | Average value: 4.83 GPa Grade Count:4 |
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 15 mm/min; ASTM D790 |
LG Chemical 20HRI GPPS Heat resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, S.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | conditioned, 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D790 |
Lucky IH-830 Acrylic, Injection Grade Similar to grade EH-910, but with higher flow for injection molding. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ISO 178 |
Solvay TECHNYL® A 221 Natural FA PA66, DRY Description: Product in development. Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. Suitable for food contact applicationsAv.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1000V PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in .. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1010FV PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1010K PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1010M PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1010RV PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas r.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1100EF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM PW1000 PEI (Europe-Africa-Middle East) Unfilled Standard flow Polyetherimide (Tg 217°C). Specific grade-colors aredesigned and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified. US FDA and Euro.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1000EF PEI Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp WB006 PBT (Europe-Africa-Middle East) LNP* THERMOCOMP* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | JIS-K-6740 |
Denka VINYKON R2015 PVC, R grade for hard extrusion A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 104 Polypropylene, Glass Reinforced, Chemically Coupled, Impact Modified, UL Data provided by the manufacturer, ComAlloy International Company.25% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1000EF PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS. US FDA and EU Food Contact compliant. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | |
Lehmann & Voss LUVOCOM® 1106-7940/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |