Mechanical Properties Metric English Comments
Flexural Modulus 3.05 GPa
442 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L0678 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Flexural Modulus 3.05 GPa
442 ksi
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin
Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be..
Flexural Modulus 3.05 GPa
442 ksi
ASTM D790-1
Ineos Styrenics 166H General Purpose Polystyrene (NAFTA)
Description: Polystyrene 166H is a high molecular weight general purpose polystyrene with good flow and crystal clarity. Polystyrene 166H offers good processing characteristics while yielding parts ..
Flexural Modulus 3.05 GPa
442 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0009E PC
LNP* STAT-KON* DD0009E is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant, Easy Molding.
Flexural Modulus 3.05 GPa
442 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL N1150 PPE+PS
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Flexural Modulus 3.05 GPa
442 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Flexural Modulus 3.05 GPa
442 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Flexural Modulus 3.05 GPa
442 ksi
ISO 178
Polyplastics Duranex® CRN7000 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50%
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 3.05 GPa
442 ksi
ISO 178
DuPont Performance Polymers Delrin® 588P NC010 Acetal (POM)
Nucleated Medium Viscosity Acetal HomopolymerInformation provided by DuPont Performance Polymers
Flexural Modulus 3.05 GPa
442 ksi
ISO 178
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Flexural Modulus 3.05 GPa
442 ksi
ASTM D790
Solvay TECHNYL® 1015CR PA6, DRY
Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding Available in: Asia Pacific Product Applications: TECHNYL® 1015CR has high fluidity and a good mould re..